The analysis of the material surface biodegradation in the petrochemical plant cooling water system
Movenko D.A., Laptev A.B., Golubev A.V., Kireev D.M. The analysis of the material surface biodegradation in the petrochemical plant cooling water system // Proceedings of VIAM. 2019. No. 7. DOI: 10.18577/2307-6046-2019-0-7-112-124. URL: https://www.viam-works.ru/en/journal/2019/7/12
Keywords
metal corrosion, bio-corrosion, bio-damage, biological factor, microorganisms, diatoms.
Abstract
The paper presents the results of a study of the impact of circulating cooling water of a petrochemical plant on steel samples for various periods of time. In addition to the electrochemical mechanism of corrosion caused by the presence of galvanic couples on the metal surface, the samples are affected by the biological factor, namely, the accumulation of simple algae contained in the circulating water and producing oxygen in the presence of sunlight. Measures to reduce the intensity of corrosion damage to steel in a petrochemical plant were proposed.
Reference list
- Kablov E.N. Klyuchevaya problema – materialy [The key problem is materials] // Tendentsii i oriyentiry innovatsionnogo razvitiya Rossii. M.: VIAM, 2015. S. 458–464.
- Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
- Javaherdashti R., Alasvand K. Biological treatment of microbial corrosion. Elsevier, 2019. 162 p.
- Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
- Kozlova L.S., Sibileva S.V., Chesnokov D.V., Kutyrev A.E. Ingibitory korrozii (obzor) [Corrosion inhibitors (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 67–75. DOI: 10.18577/2071-9140-2015-0-2-67-75.
- Pakiet M., Kowalczyk I., Leiva R. et al. Gemini surfactant as multifunctional corrosion and biocorrosion inhibitors for mild steel // Bioelectrochemistry. 2019. Vol. 128. P. 252–262.
- Vdovin S.M., Kablov E.N., Erofeev V.T., Startsev O.V. i dr. Ekonomicheskiye poteri ot biodestruktsii [Economic losses from biodegradation] // Sb. tr. Mezhdunar. nauch.-tekhn. konf. «Kompozitsionnyye stroitelnye materialy. Teoriya i praktika». Penza, 2015. S. 21–29.
- Telegdi J., Shaban A., Vastag G. Biocorrosion – Steel // Encyclopedia of Interfacial Chemistry. Surface Science and Electrochemistry. 2018. P. 28–42.
- Chesnokova M.G., Shalaj V.V., Kraus Ju.A., Mironov A.Ju. Assessment of Soil Biocorrosion Severness on the Pipeline Locations // Procedia Engineering. 2015. Vol. 113. P. 57–61.
- Bellendir L.E., Vlasov D.Yu., Durcheva V.N., Tsarovtseva I.M. Rol biofaktora v korrozii metallicheskikh i zhelezobetonnykh konstruktsiy gidrotekhnicheskikh sooruzheniy [Biofactor role in corrosion of metal and steel concrete structures of hydraulic engineering constructions] // Aviacionnye materialy i tehnologii. 2015. №S1 (38). S. 61–66. DOI: 10.18577/2071-9140-2015-0-S1-61-66.
- Arabey T.I., Beloglazov S.M. Uluchsheniye zashchitnogo deystviya grunta-modifikatora rzhavchiny na stal, korrodiruyushchuyu v morskoy vode i pod deystviyem Aspergillus niger [Improving the protective effect of the soil-modifier rust on steel, corroding in sea water and under the action of Aspergillus niger] // Praktika protivokorrozionnoy zashchity. 2010. Vyp. 1 (55). S. 17–22.
- Reformatskaya I.I., Podobayev A.N., Ashcheulova I.I., Artamonov O.Yu. i dr. Lokalnaya korroziya staley v usloviyakh ekvipotentsialnosti poverkhnosti [Local corrosion of steels under conditions of surface equipotentiality] // Praktika protivokorrozionnoy zashchity. 2011. Vyp. 3 (61). S. 55–63.
- Kablov E.N., Polyakova A.V., Vasileva A.A., Goryashnik Yu.S., Kirillov V.N. Mikrobiologicheskiye ispytaniya aviatsionnykh materialov [Microbiological testing of aviation materials] // Aviatsionnaya promyshlennost. 2011. №1. S. 35–40.
- Aktas D.F., Sorrell K.R., Duncan K.E. et al. Anaerobic hydrocarbon biodegradation and biocorrosion of carbon steel in marine enviroments: The impact of different ultra low sulfur diesels and bioaugmentation // International Biodeterioration and Biodegradation. 2017. Vol. 118. P. 45–56.
- Akhiyarov R.Zh., Laptev A.B., Ibragimov I.G. Povysheniye promyshlennoy bezopasnosti ekspluatatsii obektov neftedobychi pri biozarazhenii i vypadenii soley metodom kompleksnoy obrabotki plastovoy vody [Increase of industrial safety of operation of oil production facilities with bioinfection and salt precipitation by the method of complex treatment of formation water ] // Neftepromyslovoye delo. 2009. №3. S. 44–46.
- Krivushina A.A., Goryashnik Yu.S. Sposoby zashchity materialov i izdeliy ot mikrobiologicheskogo porazheniya (obzor) [Ways of protection of materials and products from microbiological damage (review)] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 80–86. DOI: 10.18577/2071-9140-2017-0-2-80-86.
- Laptev A.B., Navalikhin G.P. Povysheniye bezopasnosti ekspluatatsii promyslovykh nefteprovodov [Improving the safety of operating oil pipelines] // Neftepromyslovoye delo. 2006. №1. S. 48–52.
- Akhiyarov R.Zh., Matveyev Yu.G., Laptev A.B., Bugay D.E. Resursosberegayushchiye tekhnologii predotvrashcheniya biozarazheniya plastovykh vod predpriyatiy neftedobychi [Resource-saving technologies to prevent bioinfection of formation waters of oil production enterprises] // Neftegazovoye delo: elektron. nauch. zhurn. 2011. №5. S. 232–242. Available at: htt://ogbus.ru (accessed: March 29, 2019).
- Laptev A.B., Lutsenko A.N., Kurs M.G., Bukharev G.M. Opyt issledovaniy biokorrozii metallov [Experience in the study of the biocorrosion of metals] // Praktika protivokorrozionnoy zashchity. 2016. №2 (80). S. 36–57.
- Mityaseva N.A., Maksimova O.V., Georgiyev A.A. Flora makrovodorosley severnoy chasti rossiyskogo poberezhya Chernogo morya [Macro-algae flora of the northern part of the Russian Black Sea coast] // Ekologiya morya. 2003. Vyp. 64. S. 24–28.