Strain state monitoring of the structural state from polymer matrix composite material based on fiber-optic sensors (review)

Ruzakov I.A.
Ruzakov I.A. Strain state monitoring of the structural state from polymer matrix composite material based on fiber-optic sensors (review) // Proceedings of VIAM. 2019. No. 4. DOI: 10.18577/2307-6046-2019-0-4-88-98. URL: https://www.viam-works.ru/en/journal/2019/4/10
Keywords
polymer matrix composite material, fibre bragg grating, delamination, cracks, structural health monitoring.
Abstract

A large number of published articles devoted to the integration of fiber optic sensors into the structure of composite material demonstrates research and practical interest in this area. Fiber optic technology does possible to monitor the internal state of the plate from polymer matrix composite material. This allows to track the resource of individual structural elements in real-time and quickly identify defects and cracks.

This article provides an overview of modern methods for determining the impact damage of structural elements of aircraft made from polymer matrix composite material using fiber-optic Bragg gratings. The advantages of using fiber-optic sensors in the systems of embedded control of the plate from polymer matrix composites is shown.

Reference list
  1. Kablov E.N. Shestoy tekhnologicheskiy uklad [The sixth technological structure] // Nauka i zhizn. 2010. №4. S. 2–7.
  2. Doriomedov M.S., Daskovskij M.I., Skripachev S.Yu., Shein E.A. Polimernye kompozicionnye materialy v zheleznodorozhnom transporte Rossii (obzor) [Polymer composite materials in the Russian railways (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 12. Available at: http://www.viam-works.ru (accessed: October 19, 2018). DOI: 10.18577/2307-6046-2016-0-7-12-12.
  3. Kablov E.N. Osnovnyye itogi i napravleniya razvitiya materialov dlya perspektivnoy aviatsionnoy tekhniki [The main results and directions of development of materials for advanced aviation equipment] // 75 let. Aviatsionnyye materialy. M.: VIAM, 2007. S. 20–26.
  4. Timoshkov P.N., Khrulkov A.V., Yazvenko L.N. Kompozitsionnye materialy v avtomobilnoy promyshlennosti (obzor) [Composite materials in automotive industry (review)] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №6 (54). St. 07. Available at: http://www.viam-works.ru (accessed: July 19, 2018). DOI: 10.18577/2307-6046-2017-0-6-7-7.
  5. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  6. Kablov E.N., Startsev O.V., Medvedev I.M., Shelemba I.S. Volokonno-opticheskiye datchiki dlya monitoringa korrozionnykh protsessov v uzlakh aviatsionnoy tekhniki (obzor) [Fiber optic sensors for monitoring corrosion processes in units of aviation engineering (review)] // Aviacionnye materialy i tehnologii. 2017. №3 (48). S. 26–34. DOI: 10.18577/2071-9140-2017-0-3-26-34.
  7. Ilichev A.V., Raskutin A.E. Issledovanie vliyaniya koncentratora napryazhenij na napryazhenno-deformacionnoe sostoyanie ugleplastika metodom korrelyacii cifrovyh izobrazhenij [Research of stress concentrator influence on stress-strain state of carbon by digital images correlation method] // Aviacionnye materialy i tehnologii. 2014. №3. S. 62–66. DOI: 10.18577/2071-9140-2014-0-3-61-62.
  8. Startsev V.O., Mahonkov A.Yu., Kotova E.A. Mehanicheskie svojstva i vlagostojkost' PKM s povrezhdeniyami [Mechanical properties and moisture resistance of PCM with damages] // Aviacionnye materialy i tehnologii. 2015. №S1 (38). S. 49–55. DOI: 10.18577/2071-9140-2015-0-S1-49-55.
  9. Latishenko V.A., Matiss J.G., Sandalov A.V. Diagnostics of load carrying capacity of composite structures // 10th World Conference on Non-Destructive Testing. Moscow. 1982. Rep. 5–3.
  10. Murashov V.V., Gunyayev G.M., Rumyantsev A.F. Ispol'zovaniye informativnykh parametrov priborov nerazrushayushchego kontrolya pri diagnostike fiziko-mekhanicheskikh kharakteristik ugleplastikov [Use of informative parameters of devices of non-destructive testing at diagnostics of physicomechanical characteristics carbonplastics] // Aviacionnye materialy i tehnologii. M.: VIAM, 2002. Vyp.: Polimernyye kompozitsionnyye materialy. S. 70–77.
  11. Murashov V.V., Rumyantsev A.F. Diagnosis of physical and mechanical properties of constructional carbon fiber reinforced plastics (CFRP) // 10th European Conference on Non-Destructive Testing (Moscow, June 7–11, 2010). 2010. Disc 1: Reports.
  12. Ermolov I.N., Lange Yu.V. Nerazrushayushchiy kontrol: spravochnik v 7 t. [Non-destructive testing: reference book in 7 vol.] M.: Mashinostroenie, 2006. T. 3: Ultrazvukovoy kontrol. 864 s.
  13. Murashov V.V., Rumyantsev A.F. Defekty monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov i metody ikh vyyavleniya. Chast 1. Defekty monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov [Defects of monolithic parts and multilayer structures made of polymer composite materials and methods for their detection. Part 1. Defects of monolithic parts and multilayer structures made of polymer composite materials] // Kontrol. Diagnostika. 2007. №4. S. 23–31.
  14. Murashov V.V., Rumyantsev A.F. Defekty monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov i metody ikh vyyavleniya. Chast 2. Metody vyyavleniya defektov monolitnykh detaley i mnogosloynykh konstruktsiy iz polimernykh kompozitsionnykh materialov [Defects of monolithic parts and multilayer structures made of polymer composite materials and methods for their detection. Part 2. Methods for detection of defects in monolithic parts and multilayer structures made of polymer composite materials] // Kontrol. Diagnostika. 2007. №5. S. 31–42.
  15. Brand C., Boller C. Identification of life cycle cost reduction in structures with self-diagnostic devices // Proceedings of NATO RTO Symposium on Design for Low Cost Operation and Support (Ottawa, October 21–22, 1999). Raper 17.
  16. Aldridge N., Foote P.D., Read I. Operational load monitoring for aircraft and maritime applications // Strain. 2000. Vol. 36. P. 123–126.
  17. Measures R.M. Structural Monitoring with Fiber Optic Technology. 1st ed. London: Academic Press, 2004. P. 1609–1610.
  18. Chandler K., Ferguson S., Graver T. et al. On-line structural health and fire monitoring of a composite personal aircraft using an FBG sensing system // Proceedings SPIE. 2008. Vol. 6933. P. 125–131.
  19. Takeda N., Okabe Y., Kuwahara J. et al. Development of smart composite structures with small-diameter fiber Bragg grating sensors for damage detection: Quantitative evaluation of delamination length in CFRP laminates using Lamb wave sensing // Composites Science and Technology. 2005. Vol. 65. No. 15. P. 2575–2587.
  20. Coppola G. Analysis of feasibility on the use of fiber Bragg grating sensors as ultrasound detectors // Proceedings SPIE. 2001. 8th Annual Symposium on smart structures and Materials. Р. 224–232.
  21. Minakuchi S., Umehara T., Takagaki K. et al. Life cycle monitoring and advanced quality assurance of L-shaped composite corner part using embedded fiber-optic sensor // Composites Part A: Applied Science and Manufacturing. 2013. Vol. 48. P. 153–161.
  22. Takeda N., Minakuchi S., Umehara T. et al. Life cycle monitoring of curved composite parts using embedded fiber Bragg grating sensors // Advanced Materials Research. 2012. Vol. 410. P. 18–21.
  23. Guo H., Dai Y., Xiao G., Mrad N., Yao J. Interrogation of a long-period grating using a mechanically scannable arrayed waveguide grating and a sampled chirped fiber Bragg grating // Optical Letter. 2008. No. 33. P. 1635–1637.
  24. Kablov E.N., Sivakov D.V., Gulyayev I.N. i dr. Primeneniye opticheskogo volokna v kachestve datchikov deformatsii v polimernykh kompozitsionnykh materialakh [The use of optical fiber as strain sensors in polymer composite materials] // Vse materialy. Entsiklopedicheskiy spravochnik. 2010. №3. S. 10–15.
  25. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  26. Wang S.S. Delamination Crack Growth in Unidirectional Fiber-Reinforced Laminates under Static and Cyclic Loading // Composite Material: Testing and Design, ASTM STP. 1979. Vol. 674. P. 642–663.
  27. Kessler S. Piezoelectric-based in situ damage detection of composite materials for structural health monitoring systems: PhD Thesis Department of Aeronautics and Astronautics. Massachusetts: Massachusetts Institute of Technology, 2002. P. 100–112.
  28. Valdes S. Structural integrity monitoring of CFRP laminates using piezoelectric devices: PhD Thesis Department of Aeronautics. Imperial College London, 2000. P. 44–49.
  29. Chang F. Structural Health Monitoring: A Summary Report // Proceedings of the 2nd International Workshop on Structural Health Monitoring (Stanford, September 8–10, 1999). 1999. P. 244–276.
  30. Giurgiutiu V., Bao J., Zhao W. Active Sensor Wave Propagation Health Monitoring of Beam and Plate Structures // Proceedings of the 8th International SPIE Symposium on Smart Structures and Materials (Newport Beach, 2001). 2001. Vol. 4327. P. 184–213.
  31. Bar-Cohen Y. NDE of Fiber Reinforced Composite Materials // Materials Evaluation. 1986. Vol. 44. P. 446–454.
  32. Saravanos D.A., Heyliger P.R. Coupled Layerwise Analysis of Composite Beans with Embedded Piezoelectric Sensors and Actuators // Journal of Intelligent Material Systems and Structures. 1995. No. 6. P. 350–362.
  33. Saravanos D.A., Birman V., Hopkins D.A. Detection of Delaminations in Composite Beams using Piezoelectric Sensors // Proceedings of the 35th Structures, Structural Dynamics and Materials Conference of the AIAA. 1994. P. 218–223.
  34. Monnier T. Lamb waves-based impact damage monitoring of a stiffened aircraft panel using piezoelectric transducers // Journal of Intelligent Material Systems and Structures. 2006. P. 411–421.
  35. Lee B.C., Manson G., Staszewski W.J. Environmental effects on Lamb wave responses from piezoceramic sensors // Materials Science Forum. 2003. P. 195–202.
  36. Tsuda H., Lee J.R., Guan Y.S., Takatsubo J.J. Investigation of fatigue crack in stainless steel using a mobile fiber Bragg grating ultrasonic sensor // Optical Fiber Technology. 2007. No. 13. P. 209–214.
  37. Betz D.C., Thursby G., Culshaw B., Staszewski W.J. Identification of structural damage using multifunctional Bragg grating sensors: I. Theory and implementation // Smart Material and Structure. 2006. No. 15. P. 1305–1312.
  38. Perez I., Cui H.L., Udd E. Acoustic emission detection using fiber Bragg gratings // Proceedings SPIE. 2001. Vol. 4328. P. 209–215.
  39. Wu Q., Yu F., Okabe Y., Saito K., Kobayashi S. Acoustic emission detection and position identification of transverse cracks in carbon fiber–reinforced plastic laminates by using a novel optical fiber ultrasonic sensing system // Structural Health Monitoring. 2014. No. 14. P. 205–213.
  40. Kablov E.N., Startsev V.O., Inozemtsev A.A. Vlagonasyshhenie konstruktivno-podobnyh elementov iz polimernyh kompozicionnyh materialov v otkrytyh klimaticheskih usloviyah s nalozheniem termociklov [The moisture absorption of structurally similar samples from polymer composite materials in open climatic conditions with application of thermal spikes] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 56–68. DOI: 10.18577/2071-9140-2017-0-2-56-68.