The influence of homogenizing annealing regimes on the structural phase state and mechanical properties of aluminum-lithium alloy 1441 ingots
UDC
669.715:669.884
DOI
10.18577/2307-6046-2019-0-3-44-52
Article PDF (Russian)
(987.28 KB)
How to cite
Antipov V.V., Tkachenko E.A., Zaysev D.V., Selivanov A.A., Ovsyannikov B.V. The influence of homogenizing annealing regimes on the structural phase state and mechanical properties of aluminum-lithium alloy 1441 ingots // Proceedings of VIAM. 2019. No. 3. DOI: 10.18577/2307-6046-2019-0-3-44-52. URL: https://www.viam-works.ru/en/journal/2019/3/5
Keywords
Al–Li alloys, 1441 aluminum alloy, ingot structure, mechanical property, homogenizing annealing, technological plasticity, phase composition.
Abstract
The article presents the results of the study of the influence of temperature-time parameters of homogenization on the structure, phase composition and technological plasticity aluminum-lithium alloy 1441 ingots based on the Al–Li–Cu–Mg–Zr system. The phase composition of homogenized ingots was observed. In the structure of ingots after homogenization in different regimes, there are secondary microparticles of the phases: β¢ (Al3Zr), δ¢ (Al3Li) and S¢ (Al2CuMg). The particle size of these phases is from 5 to 50 nm. The two-stage homogenization regime was selected, and the temperature range of ingots hot rolling was specified, which are recommended for use in the production conditions of a modern metallurgical plant.
Reference list
- Kablov E.N. Sovremennyye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials - the basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N. VIAM: prodolzheniye puti [VIAM: the continuation of the path] // Nauka v Rossii. 2012. №11. S. 16–21.
- Kablov E.N. Strategicheskiye napravleniya razvitiya materialov i tekhnologiy ikh pererabotki na period do 2030 goda // Aviatsionnyye materialy i tekhnologii. 2012. №S. S. 7–17.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Antipov V.V. Perspektivy razvitiya alyuminievyh, magnievyh i titanovyh splavov dlya izdelij aviacionno-kosmicheskoj tehniki [Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering] // Aviacionnye materialy i tehnologii. 2017. №S. S. 186–194. DOI: 10.18577/2107-9140-2017-0-S-186-194.
- Antipov V.V., Serebrennikova N.Yu., Shestov V.V., Sidelnikov V.V. Sloistyye gibridnyye materialy na osnove listov iz alyuminiy-litiyevykh splavov [Laminated hybrid materials on basis of Al–Li alloy sheets] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 212–224. DOI: 10.18577/2071-9140-2017-0-S-212-224.
- Illarionov E.I., Kolobnev N.I., Gorbunov P.Z. Alyuminiyevyye splavy v aviakosmicheskoy tekhnike / pod obshch. red. E.N. Kablova [Aluminum alloys in aerospace / gen. ed. by E.N. Kablov]. M.: Nauka, 2001. 187 s.
- Grushko O.E., Ovsyannikov B.V., Ovchinnikov V.V. Alyuminiyevo-litiyevyye splavy: metallurgiya, svarka, metallovedeniye [Aluminum-lithium alloys: metallurgy, welding, metallurgy]. M.: Nauka, 2014. 206 s.
- Komarov S.B., Mozharovskiy S.M., Ovsyannikov B.V., Makarov G.S., Grushko O.E. Zashchita i rafinirovaniye alyuminiyevo-litiyevykh splavov flyusami [Protection and Refining of Aluminum-Lithium Alloys with Fluxes] // Tsvetnyye metally. 1995. №10. S. 57–60.
- Novikov I.I. Teoriya termicheskoy obrabotki metallov [Theory of heat treatment of metals]. M.: Metallurgiya, 1978. 392 s.
- Mondolfo L.F. Struktura i svoystva alyuminiyevykh splavov [Structure and properties of aluminum alloys]. M.: Metallurgiya, 1979. 639 s.
- Altman M.B., Andreyev G.A., Balakhontsev G.A. i dr. Plavka i litye alyuminiyevykh splavov: spravochnik. 2-ye izd. pererab. i dop. [Melting and casting of aluminum alloys: a reference book. 2nd ed. recv and add.] M.: Metallurgiya, 1983. 351 s.
- Vakhromov R.O., Tkachenko E.A., Lukina E.A., Selivanov A.A. Vliyaniye gomogenizatsionnogo otzhiga na strukturu i svoystva slitkov iz splava 1933 sistemy Al–Zn–Mg–Cu [Influence of homogenization annealing on structure and properties of ingots from 1933 alloy of Al–Zn–Mg–Cu system] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 01. Available at: http://viam-works.ru (accessed: January 14, 2019) DOI: 10.18577/2307-6046-2015-0-11-1-1.
- Belov N.A. Fazovyy sostav promyshlennykh i perspektivnykh alyuminiyevykh splavov [Phase composition of industrial and advanced aluminum alloys]. M.: MISiS, 2010. 511 s.
- Prasad N.E., Gokhale A.A., Wanhill R.J.H. Aluminum-Lithium Alloys, Processing, Properties, and Applications. Butterworth-Heinemann is an imprint of Elsevier, 2014. 531 p.
- Dobatkin V.I., Gabidullin R.M., Kolachev B.A., Makarov G.S. Gazy i okisly v alyuminiyevykh deformiruyemykh splavakh [Gases and oxides in wrought aluminum alloys]. M.: Metallurgiya, 1976. 264 s.