Abstract

The article discusses the materials of foreign and domestic publications in the field of development biodegradable materials and the manufacture of implants for medicine, in particular for the needs of orthopedics. Magnesium alloys possess the properties closest to natural bone among all biodegradable materials. The creation of biodegradable and biocompatible implants that would remain in the body only for a limited period of time that necessary to repair damage is an urgent task, the solution of which provides for the expansion of the use of magnesium alloys. The article describes the effect of alloying elements on the properties of magnesium alloys (strength and corrosion), provides methods for creating coatings that contribute to improving the corrosion resistance of implants made from magnesium alloys. The standards for the content of elements in the human body are given, the excess of which can contribute to the development of negative effects for eliminating which, it is necessary to solve the problem of optimizing the number of alloying elements in accordance with the norms of the physiological environment in the areas of implantation and monitoring the corrosion process.

Reference list
  1. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  2. Mukhina I.Yu. Struktura i svoystva novykh liteynykh magniyevykh splavov [Structure and properties of new foundry magnesium alloys] // Liteynoye proizvodstvo. 2011. №12. S. 12–14.
  3. Murugan R., Ramakrishna S. Development of nanocomposites for bone grafting // Composites Science and Technology. 2005. Vol. 65. P. 2385–2406.
  4. Ye X., Tse Z.T.H., Tang G., Song G. Mechanical properties and phase transition of biomedical titanium alloy strips with initial quasi-single phase state under highenergy electropulses // Journal of the Mechanical Behavior of Biomedical Materials. 2015. Vol. 42. P. 100–115.
  5. Kablov E.N., Bondarenko Yu.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v usloviyah vysokogradientnoj napravlennoj kristallizacii [Features of structure and heat resisting properties of monocrystals of 001> high-rhenium nickel hot strength alloys received in the conditions of high-gradient directed crystallization] // Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  6. Nochovnaya N.A., Ivanov V.I., Alekseev E.B., Kochetkov A.S. Puti optimizacii ekspluatacionnyh svojstv splavov na osnove intermetallidov titana [Ways of optimization of operational properties of alloys on the basis of titanium intermetallic compound] // Aviacionnye materialy i tehnologii. 2012. №S. S. 196–206.
  7. Rashmir-Raven A.M., Richardson D., Aberman H., De Young D.J. The response of cancellous and cortical canine bone to hydroxylapatite-coated and uncoated titanium rods // Journal of Applied Bio Materials. 1995. Vol. 6. P. 237–242.
  8. Nagels J., Stokdijk M., Rozing P.M. Stress shielding and bone resorption in shoulder arthroplasty // Journal of Shoulder and Elbow Surgery. 2003. Vol. 12. P. 35–39.
  9. Staiger M.P., Pietak A.M., Huadmai J., Dias G. Magnesium and its alloys as orthopedic biomaterials: a review // Biomaterials. 2006. Vol. 27. P. 1728–1734.
  10. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  11. Song G. Control of biodegradation of biocompatible magnesium alloys // Corrosion Science. 2007. Vol. 49. P. 1696–1701.
  12. Walker J., Shadanbaz S., Kirkland N.T. et al. Magnesium alloys: predicting in vivo corrosion with in vitro immersion testing // Journal of Biomedical Materials Research Part B: Applied Biomaterials. 2012. Vol. 100. P. 1134–1141.
  13. Wen Z., Wu C., Dai C., Yang F. Corrosion behaviors of Mg and its alloys with different Al contents in a modified simulated body fluid // Journal of Alloys and Compounds. 2009. Vol. 488. P. 392–399.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  15. Morozova G.I., Mukhina I.Yu. Nanostrukturnoye uprochneniye liteynykh magniyevykh splavov sistemy Mg–Zn–Zr [Nanostructural Hardening of Casting Mg Alloys of the Mg–Zn–Zr System] // MiTOM. 2011. №11. S. 3–7.
  16. Mukhina I.Yu. Issledovaniye metallicheskikh sistem na osnove magniya i razrabotka printsipov sozdaniya korrozionnostoykikh magniyevykh splavov [Investigation of metallic systems based on magnesium and the development of principles for the creation of corrosion-resistant magnesium alloys] // MiTOM. 2014. №1. S. 8–10.
  17. Volkova E.F., Mukhina I.Yu. Novyye materialy na magniyevoy osnove i vysokoresursnyye tekhnologii ikh proizvodstva [New materials based on magnesium and high-resource technologies for their production] // Tekhnologiya legkikh splavov. 2007. №2. S. 28–34.
  18. Mukhina I. Yu., Uridiya Z.P. Magniy – osnova sverkhlegkikh materialov [Magnesium – the basis of ultralight materials] // Metallurgiya mashinostroyeniya. 2005. №6. S. 29–31.
  19. Mukhina I.Yu., Bobryshev B.L., Antipov V.V., Koshelev A.O., Bobryshev D.B. Struktura i svoystva splavov sistemy Mg–Al–Zr pri litye v kokil' i formy iz KhTS [The structure and properties of alloys of the Mg – Al – Zr system during the casting of metal into molds and molds from HTS] // Liteynoye proizvodstvo. 2014. №8. S. 6–10.
  20. Uridiya Z.P., Mukhina I.Yu. Zakonomernosti vzaimodeystviya legiruyushchikh elementov i formirovaniye nanostrukturirovannogo sostoyaniya liteynykh magniyevykh splavov sistemy Mg–Zn–Zr [Regularities interaction of the alloying elements and nanostructured condition formation of casting magnesium alloys Mg–Zn–Zr system] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №6 (54). St. 01. Available at: http://www.viam-works.ru (accessed: December 16, 2018). DOI: 10.18577/2307-6046-2017-0-6-1-1.
  21. Mukhina I.Yu., Duyunova V.A., Uridiya Z.P. Perspektivnyye liteynyye magniyevyye splavy [Promising casting magnesium alloys] // Liteynoye proizvodstvo. 2013. №5. S. 2–5.
  22. Mukhina I.Yu., Duyunova V.A., Frolov A.V., Uridiya Z.P. Vliyaniye legirovaniya RZM na zharoprochnost' liteynykh magniyevykh splavov [Effect of alloying of rare-earth metals on the heat resistance of cast magnesium alloys] // Metallurgiya mashinostroyeniya. 2014. №5. S. 34–38.
  23. Frolov A.V., Muhina I.Yu., Leonov A.A., Uridiya Z.P. Vliyanie legirovaniya redkozemelnymi metallami na svojstva i strukturu litejnogo magnievogo splava eksperimentalnogo sostava sistemy Mg–Zr–Zn–Y–Nd [An influence of rare-earth metals doping on properties and structure of the experimental Mg–Zr–Zn–Y–Nd casting magnesium alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №3. St. 03. Available at: http://www.viam-works.ru (accessed: December 16, 2018). DOI: 10.18577/2307-6046-2016-0-3-3-3.
  24. Kazakbayeva A.A. Formirovaniye i issledovaniye mikrodugovykh Sr-soderzhashchikh kal'tsiyfosfatnykh biopokrytiy na splave Mg-0.8 Ca [Formation and study of microarc Sr-containing calcium phosphate biocoatings on Mg-0.8 Ca alloy] // Perspektivy razvitiya fundamental'nykh nauk: sb. nauch. tr. XV Mezhdunar. konf. studentov, aspirantov i molodykh uchenykh (Tomsk, 24–27 aprelya 2018 g.) v 7 t. Tomsk: Izd. Dom Tomskogo gos. un-ta, 2018. T. 2: Khimiya. S. 129–131.
  25. Wang D., Bierwagen G.P. Sol-gel coatings on metals for corrosion protection // Progress in Organic Coatings. 2009. Vol. 64. P. 327–338.
  26. Agrawal C.M. Reconstructing the human body using biomaterials // The Journal of The Minerals, Metals & Materials Society. 1998. Vol. 50. P. 31–35.