I. S. Lednev Equipment and accessories for conducting magnetic powder control of aviation materials // Proceedings of VIAM. 2026. No. 10 (164). С. 276-288. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-276-288.

Equipment and accessories for conducting magnetic powder control of aviation materials

I. S. Lednev1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article highlights current stationary flaw detectors, auxiliary equipment and accessories that allow for high-level magnetic particle inspection of aviation materials. The main elements of the accessories and the important stages of their application are highlighted. The most critical items are suitable control samples selected based on the used equipment and the methods of magnetization, which help to confirm the operability of the flaw detector and the magnetic indicator. Methods for determining the detecting capacity of several types of magnetic indicators are considered, and methods and approaches for conducting magnetic powder control of aircraft parts are described.

Keywords
magnetic non-destructive testing, magnetic particle inspection, discontinuity, aviation production, monitoring equipment, magnetic indicator



Reference list
  1. RTM 1.2A.020–2011. Non-destructive Testing. Magnetic Particle Testing of Aircraft Components. Moscow: VIAM, 2011, 95 p.
  2. Non-destructive Testing: Handbook in 7 vols. Ed. V.V. Klyuev. Moscow: Mashinostroenie, 2004, vol. 6, book 1: Magnetic Testing Methods, 832 p.
  3. Shelikhov G.S. Magnetic Particle Testing of Components and Assemblies. Moscow: NTC Expert, 1995, 224 p.
  4. Beda P.I., Vybornov B.I., Glazkov Yu.A. et al. Non-destructive Testing of Metals and Products: Handbook. Ed. G.S. Samoylovich. Moscow: Mashinostroenie, 1976, 456 p.
  5. State Standard 21105–87. Non-destructive Testing. Magnetic Particle Method. Moscow: Publ. House of Standards, 2003, 14 p.
  6. State Standard R 56512–2015. Non-destructive Testing. Magnetic Particle Method. Typical Technological Processes. Moscow: Standartinform, 2016, 56 p.
  7. State Standard R ISO 9934-2–2011. Non-destructive Testing. Magnetic Particle Method. Part 2. Flaw Detecting Materials. Moscow: Standartinform, 2013, 16 p.
  8. ASTM E1444/E1444M-16e1. Standart practice for magnetic particle testing. West Conshohocken, PA: ASTM International, 2016, 22 p.
  9. State Standard R ISO 9934-1–2011. Non-destructive testing. Magnetic particle method. Part 1. Basic requirements. Moscow: Standartinform, 2019, 16 p.
  10. Erasov V.S., Oreshko E.I. Mechanical testing and properties of structural aircraft metallic materials: textbook. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 344 p.
  11. Boychuk A.S., Dikov I.A., Generalov A.S., Yakovleva S.I. Non-destructive testing of radius zones in monolithic carbon fiber reinforced plastic (CFRP) structures using ultra-sonic phased arrays. Aviation materials and technologies, 2026, no. 1 (82), pp. 255–266. Available at: http://www.journal.viam.ru (accessed: March 10, 2026). DOI: 10.18577/2713-0193-2026-0-1-255-266.
  12. Skorobogatko D.S., Golovkov A.N., Kudinov I.I., Kulichkova S.I. Evaluation of efficiency of using water washing solutions based on different classes of surfactants for cleaning metal surfaces before carrying out capillary fluorescent penetrant testing. Aviation materials and technologies, 2023, no. 1 (70), pp. 137–147. Available at: http://www.journal.viam.ru (accessed: March 10, 2026). DOI: 10.18577/2713-0193-2023-0-1-137-147.
  13. Krasnov I.S., Lozhkova D.S., Dalin M.A. Evaluation of deficiency of titanium alloy forgings for probabilistic calculation of gas turbine engine disks fracture risk. Aviation materials and technologies, 2021, no. 2 (63), pp. 115–122. Available at: https://www.journal.viam.ru (accessed: March 10, 2026). DOI: 10.18577/2713-0193-2021-0-2-115-122.
  14. Lednev I.S. Magnetic methods of non-destructive testing of aircraft parts. Aviation materials and technologies, 2024, no. 1 (74), pp. 111–120. Available at: http://www.journal.viam.ru (accessed: March 10, 2026). DOI: 10.18577/2713-0193-2024-0-1-111-120.
  15. Gerasimov V.G., Pokrovsky A.D., Sukhorukov V.V. Non-destructive testing: in 5 books. Moscow: Higher School, 1992, book 3: Electromagnetic testing: practical manual. Ed. V.V. Sukhorukov, 312 p.