E. O. Valevin, V. O. Startsev, A. A. Skirta, M. R. Pavlov Research on changes in the glass transition temperature of fiberglass under tropical humid climate // Proceedings of VIAM. 2026. No. 7 (161). С. 226–236. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-226-236.
Research on changes in the glass transition temperature of fiberglass under tropical humid climate
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
The research presents experimental results of long-term field climatic tests of structural fiberglass based on an epoxy binder used in the aviation industry in a tropical humid climate on Hainan Island (PRC). The change in relaxation behavior of materials after exposure to tropical humid climate conditions lasting for 5 years was investigated. A comparative analysis of the obtained data with the results after exposure in a moderately warm climate (Gelendzhik, Russian Federation) was carried out.
Keywords
fiberglass, climatic tests, glass transition temperature, strength, plasticization, tropical climate
Reference list
- Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. III. Significant factors of aging. Deformatsiya i razrushenie materialov, 2011, no. 1. pp. 19–27.
- Nikolaev E.V. Maintenance of service characteristics of polymer composite materials for aircraft engine nacelles when exposed to climatic and operational factors: thesis, Cand. of Sc. (Tech.). Moscow: VIAM, 2016, 123 p.
- Sookay N.K., Klemperer C.J., Verijenko V.E. Environmental testing of advanced epoxy composites. Composite Structures, 2003, vol. 62, pp. 429–433.
- Stifel P. Effect of long term outdoor exposure on composite materials. 20th Structures, Structural Dynamics, and Materials Conference. St. Louis, 1979, pp. 273–274.
- Nishizaki I., Sasaki I., Tomiyama T. Outdoor exposure tests of pultruded CFRP plates. Proceedings of the 6th International Conference on FRP Composites in Civil Engineering (CICE 2012). Rome, 2012, paper 11-096, pp. 1–8.
- Pérez-Pacheco E., Cauchí-Cupul J.I., Valadez-González A., Herrera-Franco P.J. Effect of moisture absorption on the mechanical behavior of carbon fiber/epoxy matrix composites. Journal of Materials Science, 2013, vol. 48, pp. 1873–1882.
- Gao C., Zhou C. Moisture absorption and cyclic absorption–desorption characters of fibre-reinforced epoxy composites. Journal of Materials Science, 2019, vol. 54, no. 11, pp. 8289–8301.
- Veligodskiy I.M., Koval T.V., Kurnosov A.O., Marakhovskiy P.S. Study of resistance of glass fiber reinforced plastic to natural weathering in different climatic conditions. Trudy VIAM, 2022, no. 11 (117), pp. 134–148. Available at: http://www.viam-works.ru (accessed: September 27, 2025). DOI: 10.18577/2307-6046-2022-0-11-134-148.
- Kirillov V.N., Efimov V.A. Problems of studying the climatic resistance of aviation non-metallic materials. 75 years. Aviation materials. Selected works of «VIAM». Moscow: VIAM, 2007, pp. 379–388.
- Liu X., Su Q., Zhu J., Song X. The Aging Behavior and Life Prediction of CFRP Rods under a Hygrothermal Environment. Polymers, 2023, vol. 15, no. 11, art. 2490.
- Startsev V.O., Startsev O.V., Zeleneva T.O., Vardanyan A.M. Influence of precipitation on changes in the mass of samples of polymeric composite materials in open climatic conditions. Aviation materials and technologies, 2024, no. 1 (74), pp. 136–154. Available at: http://www.journal.viam.ru (accessed: September 27, 2025). DOI: 10.18577/2713-0193-2024-0-1-136-154.
- Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. I. Aging mechanisms. Deformatsiya i razrusheniye materialov, 2010, no. 11, pp. 19–27.
- Kablov E.N., Startsev O.V., Krotov A.S., Kirillov V.N. Climatic aging of composite materials for aviation purposes. II. Relaxation of the initial structural nonequilibrium and the gradient of properties across the thickness. Deformatsiya i razrusheniye materialov, 2010, no. 12, pp. 40–46.
- Heinrich M., Crawford B., Milani A.S. Degradation of Fibreglass Composites under Natural Weathering Conditions. MOJ Polymer Science, 2017, vol. 1, no. 1, pp. 18–24.
- Kirillov V.N., Startsev O.V., Efimov V.A. Climatic firmness and damageability of polymeric composite materials, problems and solutions. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 412–423.
- Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials: textbook. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
- Bonniau P., Bunsell A.R. A comparative study of water absorption theories applied to glass epoxy composites. Journal of Composite Materials, 1981, vol. 15, no. 5, pp. 272–293.
- Kirillov V.N., Kavun N.S., Rakitina V.P. et al. Studies of the influence of heat and humidity on the properties of epoxy fiberglass. Plasticheskie massy, 2008, no. 9, pp. 14–17.
- Ageing of composites. Ed. R. Martin. Cambridge: Woodhead Publishing Limited, 2008, 544 p.
- Startsev O.V., Perepechko I.I., Startseva L.T., Mashinskaya G.P. Structural changes in plasticized cross-linked amorphous polymer. Vysokomolekulyarnye soviedineniya. Ser.: B, 1983, vol. 25, no. 6, pp. 457–461.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: November 14, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Mitsushima H. Strength degradation of GFRP by water. Proceedings of 22 Congress of Materials Research. Kyoto, 1979, pp. 241–245.
- Startsev V.O., Plotnikov V.I., Antipov Yu.V. Reversible influence of moisture on the mechanical properties of PCM after weathering. Trudy VIAM, 2018, no. 5 (65), pp. 110–118. Available at: http://www.viam-works.ru (accessed: September 09, 2025). DOI: 10.18577/2307-6046-2018-0-5-110-118.
- Startsev O.V., Skirta A.A., Startsev V.O., Valevin E.O., Dvirnaya E.V. Comparison of the properties of carbon fiber reinforced plastics and glass fiber reinforced plastics based on the VSE-1212 binder after exposure to different climatic zones. Trudy VIAM, 2024, no. 7 (137), pp. 77–92. Available at: http://www.viam-works.ru (accessed: September 09, 2025). DOI: 10.18577/2307-6046-2024-0-7-77-92.