A. V. Alekseev, P. V. Yakimovich Determination of impurities in tantalum by high-resolution glow discharge mass spectrometry // Proceedings of VIAM. 2026. No. 7 (161). С. 193–202. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-193-202.

Determination of impurities in tantalum by high-resolution glow discharge mass spectrometry

A. V. Alekseev1, P. V. Yakimovich1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

In this work the impurities of 36 elements in tantalum by high-resolution glow discharge mass spectrometry (GDMS) were determined. The sample preparation for analysis is described. The corresponding equipment settings were selected to achieve maximum analytical signals from all target elements. Spectral interferences were eliminated by using high resolution. Relative sensitivity coefficients were calculated for all determined elements using X-ray fluorescence spectroscopy.

Keywords
high resolution glow discharge mass spectrometry, GDMS, tantalum, nickel alloys, determination of harmful impurities
Reference list
  1. Omarova D.K. Application of tantalum and production of world tantalum products. Byulleten VSNTS SO RAMN, 2012, no. 1 (83), pp. 143–148.
  2. Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), pp. 3–12. Available at: http://www.viam-works.ru (accessed: December 04, 2025). DOI: 10.18577/2307-6046-2020-0-3-3-12.
  3. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  4. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: December 04, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  5. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), pp. 3–13. Available at: http://www.journal.viam.ru (accessed: December 04, 2025). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  6. Min P.G., Vadeev V.E., Kramer V.V. The development of the new VZhM200 superalloy and the technology of its production for casting of the advanced engines' blades by the directional crystallization. Aviation materials and technologies, 2021, no. 3 (64), pp. 11–18. Available at: http://www.journal.viam.ru (accessed: December 04, 2025). DOI: 10.18577/2713-0193-2021-0-3-11-18.
  7. Gromov V.I., Yakusheva N.A., Vostrikov A.V., Cherkashneva N.N. High strength structural steels for gas-turbine engine shafts (review). Aviation materials and technology, 2021, no. 1 (62), pp. 3–12. Available at: http://www.journal.viam.ru (accessed: December 04, 2025). DOI: 10.18577/2713-0193-2021-0-1-3-12.
  8. Kablov E.N., Chabina E.B., Morozov G.A., Muravskaya N.P. Conformity assessment of new materials using high-level CRMs and MI. Kompetentnost, 2017, no. 2, pp. 40–46.
  9. State Standard 18904.1–89. Tantalum and its oxide. Photometric method for determining molybdenum and tungsten. Moscow: Publ. House of Standards, 1989, pp. 6–9.
  10. Luke C.L. Spectrophotometric determination of niobium in tantalum metal. Analytical Chimica Acta, 1966, vol. 34, pp. 165–168.
  11. Hasegawa S., Kobayashi T., Ide K., Hasegawa R. Determination of trace amounts of sodium and potassium in high-purity tantalum by graphite-furnace atomic absorption spectrometry. Bunseki Kagaku, 1993, vol. 42 (10), pp. 643–647.
  12. State Standard 18904.6–89. Tantalum and its oxide. Spectral method for determination of aluminum, vanadium, iron, calcium, silicon, magnesium, manganese, copper, nickel, niobium, tin, titanium, chromium, and zirconium. Moscow: Publ. House of Standards, 1989, pp. 12–16.
  13. Filippov M.N., Mezhevaya L.Yu., Baranovskaya V.B. Modern trends in the application and analytical control of niobium and tantalum. Analitika veshchestvi i materialov, 2023, vol. 13, no. 5, pp. 366–378.
  14. Grebneva O.N., Kubrakova I.V., Kudinova T.F., Kuzmin N.M. Direct determination of trace elements in niobium, tantalum and their oxides by inductively coupled plasma atomic emission spectrometry after microwave dissolution. Spectrochimica Acta Part B, 1997, vol. 52, pp. 1151–1159.
  15. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS. Mikrochimica Acta, 2001, vol. 137, pp. 149–155.
  16. Pupyshev A.A., Epova E.N. Spectral interference of polyatomic ions in the method of mass spectrometry with inductively coupled plasma. Analitika i kontrol, 2001, vol. 5, no. 4, pp. 335–369.
  17. Kozono S., Sakamoto H., Takashi R., Haraguchi H. Multielement determination of ultratrace impurities in high purity tantalum metals by flow injection/inductively coupled plasma mass spectrometry. Analytical Sciences, 1998, vol. 14 (4), pp. 757–762.
  18. Jakubowski N., Prohaska T., Rottmann L., Vanhaecke F. Inductively coupled plasma- and glow discharge plasma-sector field mass spectrometry. Part I. Tutorial: Fundamentals and instrumentation. Journal of Analytical Atomic Spectrometry, 2011, vol. 26, pp. 693–726.
  19. Ganeev A.A., Gubal A.R., Uskov K.N., Potapov S.V. Analytical mass spectrometry with glow discharge. Izvestiya Akademii nauk. Seriya khimicheskaya, 2012, no. 4, pp. 1–15.