A. V. Leonov, N. M. Voznesenskaya, A. V. Knyazev, E. I. Ulyanov Influence of heat treatment on the corrosion resistance of high‑strength corrosion‑resistant martensitic steel with super‑equilibrium nitrogen content // Proceedings of VIAM. 2026. No. 7 (161). С. 3–15. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-3-15.

Influence of heat treatment on the corrosion resistance of high‑strength corrosion‑resistant martensitic steel with super‑equilibrium nitrogen content

A. V. Leonov1, N. M. Voznesenskaya1, A. V. Knyazev1, E. I. Ulyanov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The influence of various heat treatment modes of high nitrogen martensitic corrosion-resistant steel of grade 30H15AMF-ShPD (VNS78-ShPD) on the corrosion resistance of the steel in tough test conditions is considered. The effect of different quenching and tempering temperatures on the microstructure, hardness and corrosion properties of the steel is studied.

Keywords
high nitrogen corrosion-resistant steel, corrosion resistance, quenching, tempering, heat treatment, microstructure, hardness
Reference list
  1. On the Strategy for Scientific and Technological Development of the Russian Federation: Decree of the President of the Russian Federation of February 28, 2024, No. 145. Available at: www.pravo.gov.ru (accessed: May 04, 2026).
  2. Voznesenskaya N.M., Izotov V.I., Ulyanova N.V. et al. Structure and Properties of High-Strength Stainless Steel 1Kh15N4AM3. Metallovedenie i termicheskaya obrabotka metallov, 1971, no. 1, pp. 32–35.
  3. Potak Ya.M. High-Strength Steels. Moscow: Metallurgy, 1972, 208 p.
  4. Laptev A.B., Zakirova L.I. Zagorskikh O.A., Pavlov M.R. Methods of investigation of the processes of corrosion-mechanical destruction and hydrogenation of metals (review). Part 1. Investigation of corrosion-mechanical destruction of steels. Trudy VIAM, 2022, no. 4 (110), pp. 118–130. Available at: http://www.viam-works.ru (accessed: May 04, 2026). DOI: 10.18577/2307-6046-2022-0-4-118-130.
  5. Zyryanov A.O., Vyboishchik M.A., Ioffe A.V. Influence of microstructure and heat treatment on the resistance of steels to carbon dioxide corrosion. Metallovedenie i termicheskaya obrabotka metallov, 2019, no. 2 (764), pp. 39–45.
  6. Kiseleva S.K., Zaripov N.G. Influence of severe plastic deformation on the microstructure and tribological properties of 110Kh18M-ShVD steel. Evraziyskiy Soyuz Uchenykh, 2020, no. 7-1 (76), pp. 32–36.
  7. Sevalnev G.S., Vostrikov A.V., Nefedkin D.Yu., Moiseenkov V.V., Volkov R.B., Ulyanov E.I. Study of the structure, distribution of carbide phase, hardness and tribotechnical characteristics of high-chromium bearing steels of the martensitic class. Trudy VIAM, 2023, no. 10 (128), pp. 13–23. Available at: http://www.viam-works.ru (accessed: May 04, 2026). DOI: 10.18577/2307-6046-2023-0-10-13-23.
  8. Petrov N.I., Lavrentyev Yu.L. Ways to Improve the Reliability and Service Life of Bearing Assemblies of Rotor of Modern Gas Turbine Engines and Gearboxes. Vestnik Samarskogo gosudarstvennogo aerokosmicheskogo universiteta, 2015, vol. 14, no. 3, part 1, pp. 228–237.
  9. Zaitsev A.M., Korostashevsky R.V. Operation of Aircraft Rolling Bearings. Moscow: Transport, 1968, 224 p.
  10. State Standard 5949–2018. Metal products from stainless steels and iron-nickel-based alloys, corrosion-resistant, heat-resistant, and heat-resistant. Specifications. Moscow: Standartinform, 2019, 32 p.
  11. Ooi S. A new index to estimate the corrosion resistance of aluminium-containing steel. Materials and Corrosion, 2024, vol. 75, no. 7, pp. 902–913.
  12. Gavriljuk V.G., Berns H. High nitrogen steels: structure, properties, manufacture, applications. Springer Science & Business Media, 1999, 378 p.
  13. Gudremon E. Special Steels: in 2 vols. Ed. A.S. Zaimovsky, M.L. Bernstein. Moscow: Metallurgizdat, 1959, vol. 1, 952 p.
  14. Jiang Z.H., Zhu H.C., Li H.B. et al. Pressurized metallurgy for high performance special steels and alloys. IOP Conference Series: Materials Science and Engineering, 2016, vol. 143, no. 1, p. 012038.
  15. Shlyamnev A.P., Uglov V.A., Filippov G.A. et al. Nitrogen-Based Stainless Steels: Structure, Properties, and Production Technology. Chernaya metallurgiya, 2013, no. 2, p. 12.
  16. Trojahn W., Streit E., Chin H.A., Ehlert D. Progress in bearing performance of advanced nitrogen alloys stainless steel, Cronidur 30. ASTM Special Technical publication, 1998, vol. 1327, pp. 447–459.
  17. Data sheet Cronidur® 30. Mat. no.: 1.4108. Energietechnik Essen GmbH, 2012. Available at: engineering.com (accessed: May 04, 2026).
  18. Svyazhin A.G., Kaputkina L.M. Nitrogen-Based and High-Nitrogen-Based Steels. Industrial Technologies and Properties. Izvestiya vysshikh uchebnykh zavedeniy. Chernaya metallurgiya, 2019, vol. 62, no. 3, pp. 173–187.
  19. Moiseenkov V.V., Sevalnev G.S., Volkov R.B., Dulnev K.V., Levin E.A. Application of the rotational forging method for the production of bars from high-nitrogen steel VNS-78. Aviation materials and technologies, 2022, no. 4 (69), pp. 3–15. Available at: http://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/27-13-0193-2022-0-4-3-15.
  20. High-Strength Corrosion-Resistant Steel: pat. 2725766 Rus. Federation; appl. 23.05.19; publ. 25.06.20.
  21. Dulnev K.V., Sevalnev G.S., Pahomkina T.N., Buzenkov A.V. Study of changes in microstructure, grain size and nitrogen concentration depending on heat treatment temperature of high-strength structural high-nitrogen steel. Aviation materials and technologies, 2025, no. 3 (80), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/27-13-0193-2025-0-3-3-14.