UDC
620.179.1
DOI
10.18577/2307-6046-2026-0-10-235-246
Article PDF (Russian)
(915.25 KB)
How to cite
S. S. Pichugin, E. I. Kosarina, R. R. Akbulatov, P. V. Panin Application of the eddy current method for estimating residual stresses over the depth of intermetallic TiAl-alloy parts obtained using additive technologies // Proceedings of VIAM. 2026. No. 10 (164). С. 235-246. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-235-246.
Application of the eddy current method for estimating residual stresses over the depth of intermetallic TiAl-alloy parts obtained using additive technologies
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
The article demonstrates the fundamental possibility of obtaining the electrical conductivity distribution of TiAl alloy samples made by selective electron beam melting using the eddy current method of non-destructive testing. The X-ray diffraction was performed to correlate the electrical conductivity of the samples with the residual stresses. The dependences of mechanical stresses with the depth of the studied samples before and after the application of hot isostatic pressing were shown.
Keywords
eddy current testing, surface eddy current probe, mathematical modeling, property evaluation, structuroscopy, additive manufacturing, electron beam melting, hot isostatic pressing
Reference list
- Kablov E.N., Evgenov A.G., Bakradze M.M., Nerush S.V., Krupnina O.A. New-generation materials and digital additive manufacturing technologies for critical components at FSUE VIAM. Part 2. Compensation and control of deviations, HIP, and heat treatment. Elektrometallurgiya, 2022, no. 2, pp. 2-12.
- Bakradze M.M., Peskova A.V., Kaplansky Yu.Yu. Influence of thermal post-treatment on the texture and anisotropy of mechanical properties in the Cu-Cr construction alloy manufactured by laser powder bed fusion. Aviation materials and technologies, 2022, no. 1 (66), pp. 3-16. Available at: http://www.journal.viam.ru (accessed: May 17, 2026). DOI: 10.18577/2713-0193-2022-0-1-3-16.
- Impey S., Saxena P., Salonitis K. Selective Laser Sintering Induced Residual Stresses: Precision Measurement and Prediction. Journal of Manufacturing and Materials Processing, 2021, vol. 5, is. 3, pp. 1-16. DOI: 10.3390/jmmp503010.
- Bian P., Jammal A., Xu K. et al. A Review of the Evolution of Residual Stresses in Additive Manufacturing During Selective Laser Melting Technology. Materials, 2025, vol. 18, is. 8, pp. 1-21. DOI: 10.3390/ma1808170.
- Schajer G., Ruud C. Overview of Residual Stresses and their measurement. Practical Residual stress: measurement methods. Ed. G.S. Schajer. John Wiley and Sons Ltd, 2013, pp. 1-27. DOI: 10.1002/248023.2ch1.
- Segovia R., Garcia F., Papaelias M. Review on additive manufacturing and non-destructive testing. Journal of Manufacturing Systems, 2023, vol. 66, pp. 260-286.
- Bartlett J.L., Li X. An overview of residual stresses in metal powder bed fusion. Additive Manufacturing, 2019, vol. 27, pp. 131-149.
- Nabin B., Muhammad J., Nithin R., Sekhar R. A review of the residual stress generation in metal additive manufacturing: analysis of cause, measurement, effects, and prevention. Micromachines, 2023, vol. 14, is. 7, pp. 1-30. DOI: 10.3390/MI14071480.
- Tillmann W., Schaak C., Nellesen J. et al. Hot isostatic pressing of IN718 components manufactured by selective laser melting. Additive Manufacturing, 2017, vol. 13, pp. 93-102.
- Yamamoto Y., Fujikawa T. Mechanical Properties of Ti-6Al-4V Materials Prepared by Additive Manufacturing. Technology and HIP Process. Proceedings of 11th International Conference on Hot Isostatic Pressing. Stockholm, 2014, pp. 398-404.
- Panin P.V., Lukina E.A., Bogachev I.A., Naprienko S.A. Influence of selective electron beam melting process parameters on the chemical composition, microstructure, and porosity of a Ti-Al-V-Nb-Cr-Gd system TiAl alloy. Metallurg, 2023, no. 5, pp. 54-66.
- Vastola G., Zhang G., Pei Q.X., Zhang Y. Controlling of residual stress in additive manufacturing of Ti6Al4V by finite element modeling. Additive Manufacturing, 2016, vol. 12, pp. 231-239.
- Movenko D.A., Shurtakov S.V. Microcrack formation and controlling in nickel superalloys processed by selective laser melting (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 43-51. Available at: http://www.journal.viam.ru (accessed: May 17, 2026). DOI: 10.18577/2713-0193-2022-0-2-43-51.
- Marakhovskij P.S., Barinov D.Ya., Shorstov S.Yu., Vorobev N.N. On creation of physical and mathematical models of heat and mass transfer during manufacturing by additive technologies (review). Aviation materials and technologies, 2022, no. 2 (67), pp. 111-119. Available at: http://www.journal.viam.ru (accessed: May 17, 2026). DOI: 10.18577/2713-0193-2022-0-2-111-119.
- Monakhov A.D., Yakovlev N.O., Shershak P.V. Methods for the formation of objects with artificially created residual stresses. Aviation materials and technologies, 2023, no. 4 (73), pp. 122-132. Available at: http://www.journal.viam.ru (accessed: May 17, 2026). DOI: 10.18577/2713-0193-2023-0-4-122-132.
- Gerasimov V.G., Klyuev V.V., Shaternikov V.E. Methods and Instruments for Electromagnetic Testing. Ed. V.E. Shaternikov. Moscow: Spektr, 2010, 256 p.
- Gerasimov V.G., Pokrovsky A.D., Sukhorukov V.V. Nondestructive Testing: in 5 books. Moscow: Vysshaya Shkola, 1992, book 3: Electromagnetic Testing. Ed. V.V. Sukhorukov, 312 p.
- Fedosenko Yu.K., Shkatov P.N., Efimov A.G. Eddy-Current Testing. Moscow: Spektr, 2014, 224 p.
- Kekalo I.B. Physical Properties of Metals. Section: Electrical Properties: Laboratory Manual. Moscow, 1998, 139 p.
- Shitikov V.S., Pichugin S.S. Estimation of electrical properties distribution under elastic deformation of the control object by eddy current method. Trudy VIAM, 2024, no. 11 (141), pp. 89-99. Available at: http://www.viam-works.ru (accessed: May 17, 2026). DOI: 10.18577/2307-6046-2024-0-11-89-99.
- Dorofeev A.L., Lyubashev G.A., Ostanin Yu.Ya. Measurement of Coating Thickness Using Eddy Currents. Moscow: Mashinostroenie, 1975, 64 p.
- Theodoulidis T. End effect modelling in eddy current tube testing with bobbin coils. International Journal of Applied Electromagnetics and Mechanics, 2004, vol. 19, pp. 207-212.
- Bowler J.R., Theodoulidis T.P. Coil impedance variation due to induced current at the edge of a conductive plate. Journal of Physics D: Applied Physics, 2006, vol. 39, pp. 2862-2868.
- Zec M., Uhlig R.P., Ziolkowski M., Brauer H. Finite element analysis of nondestructive testing eddy current problems with moving parts. IEEE Transactions on Magnetics, 2013, vol. 49, pp. 4785-4794.
- Paul S., Bird J.Z. Analytic 3-D eddy current model of a finite width conductive plate including edge-effects. International Journal of Applied Electromagnetics and Mechanics, 2014, vol. 45, pp. 535-542. DOI: 10.3233/jae-141874.
- Xie Y., Li J., Tao Y. et al. Edge Effect Analysis and Edge Defect Detection of Titanium Alloy Based on Eddy Current Testing. Applied Sciences, 2020, vol. 10, p. 15. DOI: 10.3390/app10248796.
- Lv C., Liu W., Jiang Y., Zhao H. Analytical modelling for edge effects and impedance characteristics of the transverse eddy current displacement sensors with rectangular coils. International Journal of Applied Electromagnetics and Mechanics, 2014, vol. 46, pp. 823-834. DOI: 10.3233/jae-130060.
- Titanium intermetallic-based alloy and article made therefrom: pat. 2606368 Rus. Federation; appl. 15.10.15; publ. 10.01.17.
- Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Titanium- and Nickel-Based Intermetallic Alloys. Ed. E.N. Kablov. 2nd ed., rev. and add. Moscow: VIAM, 2019, 316 p.
- Panin P.V., Bogachev I.A., Smirnov A.V., Lukina E.A. Quantitative analysis of porosity in a Ti-Al-V-Nb-Cr-Gd system TiAl alloy after selective electron beam melting and hot isostatic pressing. Metallurg, 2025, no. 11, pp. 66-71. DOI: 10.52351/00260827_2025_11_66.
- Akbulatov R.R., Efremova A.P., Bogachev I.A., Panin P.V. Study of isothermal phase transformations kinetics in heat-resistant alloys based on gamma titanium aluminide TiAl. Trudy VIAM, 2024, no. 11 (141), pp. 22-32. Available at: http://www.viam-works.ru (accessed: May 17, 2026). DOI: 10.18577/2307-6046-2024-0-11-22-32.
- Shitikov V.S., Pichugin S.S., Akbulatov R.R., Panin P.V. Features of the eddy current method assessment of properties parts made of intermetallic TiAl alloy, obtained using additive technologies. Trudy VIAM, 2025, no. 11 (153), pp. 124-134. Available at: http://www.viam-works.ru (accessed: May 17, 2026). DOI: 10.18577/2307-6046-2025-0-11-124-134.
The article was submitted
2026-08-26
approved and accepted for publication after reviewing
2026-08-31