D. A. Melnikov, A. Yu. Albagachiev, A. A. Rybin, A. V. Slavin Theoretical foundations of the application of vibration technologies in the manufacture of fiberglass pipes // Proceedings of VIAM. 2026. No. 10 (164). С. 133-145. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-133-145.

Theoretical foundations of the application of vibration technologies in the manufacture of fiberglass pipes

D. A. Melnikov1, A. Yu. Albagachiev2, A. A. Rybin1, A. V. Slavin1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
2Mechanical Engineering Research Institute of the Russian Academy of Sciences, Moscow, Russia; info@imash.ru

Abstract

This article is devoted to the production of three-layer fiberglass pipes using continuous winding with low-frequency vibration applied to the mandrel. A set of physical models describing the influence of vibration parameters on structure-formation processes and curing kinetics is substantiated. It is shown that selection frequency and amplitude of vibration allows for a significant reduction in residual porosity without compromising the homogeneity of the composite. The developed approach provides a scientific basis for the engineering design of vibration modules and ensures improved quality, reliability, and competitiveness of pipe products with minimal additional energy consumption.

Keywords
fiberglass pipes, winding, vibration technologies, tooling, thixotropy, degassing, porosity



Reference list
  1. Kablov E.N. New-Generation Materials and Digital Technologies for Their Processing. Vestnik Rossiskyy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), pp. 81–92. Available at: http://www.viam-works.ru (accessed: July 20, 2026). DOI: 10.18577/2307-6046-2022-0-11-81-92.
  3. Kablov E.N., Antipov V.V. The Role of New-Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiskyy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: July 20, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), pp. 61–81. Available at: http://www.journal.viam.ru (accessed: July 20, 2026). DOI: 10.18577/2713-0193-2023-0-1-61-81.
  6. Sutubalov A.I., Podzhivotov N.Yu., Shershak P.V., Yakovlev N.O. Evaluation of homogeneity of physical and mechanical properties of semi-finished products for aviation purpose. Aviation materials and technologies, 2024, no. 1 (74), pp. 121–135. Available at: http://www.journal.viam.ru (accessed: July 20, 2026). DOI: 10.18577/2713-0193-2024-0-1-121-135.
  7. Kagan D.F. Plastic Pipelines. Moscow: Khimiya, 1980, 295 p.
  8. Ivanov S.V. Fiberglass-reinforced plastic: a composite material for pipes. Truboprovody i ekologiya, 2001, no. 2, p. 7.
  9. Antoshin V.A., Melnikov D.A., Ivanov S.V., Albagachiev A.Yu. Determination of long-term strength properties of glass-composite pipes for service life calculation. Fundamental Research and Innovative Technologies in Mechanical Engineering: Proceedings of the VII Int. Sci. Conf. Moscow, 2021, pp. 29–30.
  10. Bogdanov V.V., Torner R.V. Polymer Blending. Leningrad: Khimiya, 1979, 192 p.
  11. Yang X., Zhan L., Peng Y. et al. Interface controlled micro- and macro-mechanical properties of vibration processed carbon fiber/epoxy composites. Polymers, 2021, vol. 13, no. 16, art. 2764. DOI: 10.3390/polym13162764.
  12. Kunnos G.Ya. Vibration Technology for Concrete. Leningrad: Stroyizdat, 1967, pp. 134–150.
  13. Eskin G.I. Development of Ultrasonic Melt Treatment: My 45 Years at VILS. Tekhnologiya legikh galvan, 2021, no. 3, pp. 61–71. DOI: 10.24412/0321-4664-2021-3-61-71.
  14. Belousov A.P., Belousov P.Ya., Borynyak L.A. Determination of Bubble Velocity and Size in Two-Phase Flows Using a Laser Doppler Anemometer. Avtometriya, 2015, vol. 51, no. 6, pp. 47–51.
  15. Liu Z., Wang H., Chen Y. et al. Study on Curing Kinetics and the Mechanism of Ultrasonic Curing of an Epoxy Adhesive. Polymers, 2022, vol. 14, no. 3, art. 512. DOI: 10.3390/polym14030512.
  16. Blaznov A.N., Khodakova N.N., Samoilenko V.V. et al. Investigation of various winding patterns for products based on basalt and glass rovings. Yuzhno-Sibirskiy nauchnyy vestnik, 2016, no. 4 (16), p. 9.
  17. Wallenberger F.T., Bingham P.A. Fiberglass and Glass Technology: Energy-Friendly Compositions and Applications. Springer, 2009, p. 474.
  18. Gaidachuk O., Kondratiev A., Taranenko I. et al. Method of winding of small-diameter pipes using vibration effects. Energy and Sustainability II, Lecture Notes in Mechanical Engineering, vol. 261, Springer, 2023, pp. 175–184. DOI: 10.1007/978-3-031-46874-2_16.
  19. Basov N.I., Lyubartovich S.A., Lyubartovich V.A. Vibroforming of polymers. Leningrad: Khimiya, 1979, 159 p.
  20. Balchugov A.V., Badenikov A.V., Baranova A.A. Criterion equation for the sedimentation process in the transition regime. Vestnik AGTU, 2023, vol. 1, no. 17, pp. 8–10.