O. N. Bityutskaya, N. V. Petrushin, E. M. Visik, N. A. Lonskaya, V. V. Avdeev, A. V. Vostrikov Structure formation during casting and thermal treatment of a nickel-based superalloy with reduced rhenium content for turbine blades // Proceedings of VIAM. 2026. No. 10 (164). С. 33-53. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-10-33-53.

Structure formation during casting and thermal treatment of a nickel-based superalloy with reduced rhenium content for turbine blades

O. N. Bityutskaya1, N. V. Petrushin1, E. M. Visik1, N. A. Lonskaya1, V. V. Avdeev1, A. V. Vostrikov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

A regression model has been developed for the new carbon-containing nickel-based superalloy VZhL22 with 2 wt.% Re to predict the effect of casting process parameters on the grain size in polycrystalline castings. The structure forming features of the alloy in polycrystalline and single-crystal castings and turbine blades were investigated during casting and heat treatment. The macro- and microstructures formed during casting and heat treatment provide enhanced short-term strength and long-term strength creep characteristics for polycrystalline castings.

Keywords
carbon-containing nickel-based superalloys, rhenium, casting process parameters, grain size, polycrystalline and single-crystal turbine blade castings, heat treatment, macro- and microstructures, mechanical properties

Reference list
  1. Walston S., Cetel A., MacKay R. et al. Joint development of a fourth generation single crystal superalloy. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 15–24.
  2. Koizumi Y., Kobayashi T., Yokokawa T. et al. Development of next-generation Ni-base single crystal superalloys. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 35–43.
  3. Aviation Materials: Handbook in 13 vols. Ed. E.N. Kablov. 7th ed., revised and expanded. Moscow: NRC «Kurchatov Institute» – VIAM, 2022. Vol. 3: Nickel-Based Heat-Resistant Casting Alloys and Intermetallic Alloys, 192 p.
  4. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaew M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: July 10, 2026). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  5. Elyutin E.S. Development of high-temperature nickel-based alloys of generations V and VI with enhanced long-term strength for single-crystal blades of advanced aircraft gas turbines: thesis, abstract Cand. Sc. (Tech.). Moscow, 2023, 27 p.
  6. Ni-base superalloy and gas turbine component using the same: pat. US 2010/0047110 A1; appl. 09.08.09; publ. 25.02.10.
  7. Nickel-base superalloy for high temperature, high strain application: pat. US 6632299 B1; appl. 19.10.00; publ. 14.10.03.
  8. High ductility nickel alloy directional casting of parts for high temperature and stress operation: pat. US 4461659; appl. 24.06.81; publ. 24.07.84.
  9. Low carbon directional solidification alloy: pat. US 5069873; appl. 14.08.89; publ. 03.12.91.
  10. Hochtemperaturbeständiges Bauteil aus einkristalliner oder polykristalliner Nickel-Basis Superlegierung: pat. EP 1319729 B1; appl. 13.12.01; publ. 11.04.07.
  11. High-strength and high-ductility Ni-base superalloys, parts using them, and method of producing the same: pat. EP 1795621 A1; appl. 06.12.06; publ. 13.06.07.
  12. Ospennikova O.G. Tendencies of development of heat-resistant nickel alloys of low density with polycrystalline and single-crystal structures (review). Aviacionnye materialy i tehnologii, 2016, no. 1 (40), pp. 3-19. DOI: 10.18577/2071-9140-2016-0-1-3-19.
  13. Kablov E.N., Petrushin N.V. Computer-aided design method for cast heat-resistant nickel-based alloys. Cast Heat-Resistant Alloys. The S.T. Kishkin Effect. Moscow: Nauka, 2006, pp. 56-78.
  14. Nickel-based cast heat-resistant alloy and an article made therefrom: pat. RU 2530932 C1; appl. 29.10.13; publ. 20.10.14.
  15. Petrushin N.V., Bityutskaya O.N., Visik E.M., Chabina E.B. Structural characteristics of monocrystalline castings and mechanical properties of nickel-based superalloys with low renum content. Part 2. Trudy VIAM, 2026, no. 3 (157), pp. 3-22. Available at: http://www.viam-works.ru (accessed: July 16, 2026). DOI: 10.18577/2307-6046-2026-0-3-3-22.
  16. Cast Blades for Gas Turbine Engines: Alloys, Technologies, and Coatings. Ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
  17. Logunov A.V. Heat-Resistant Nickel Alloys for Gas Turbine Blades and Disks. Rybinsk: Gazoturbinnye Tekhnologii, 2017, 854 p.
  18. Golikov I.N., Maslenkov S.B. Dendritic Segregation in Steels and Alloys. Moscow: Metallurgiya, 1977, 224 p.
  19. Bityutskaya O.N., Petrushin N.V., Visik E.M., Kuzmina N.A., Lonskaya N.A. Structural characteristics of monocrystalline castings and mechanical properties of nickel-based superalloys with low renum content. Part 1. Trudy VIAM, 2026, no. 1 (155), pp. 3-18. Available at: http://www.viam-works.ru (accessed: July 15, 2026). DOI: 10.18577/2307-6046-2026-0-1-3-18.
  20. Parker E.R., Washburn J. The role of boundaries in creep phenomena. Creep and Recovery. Trans. from Engl. ed. by A.G. Rakshstadt. Moscow: State Scientific and Technical Publishing House of Literature on Ferrous and Non-Ferrous Metallurgy, 1961, pp. 260-285.
  21. Movchan B.A. Grain boundaries in cast metals and alloys. Kyiv: Tekhnika, 1970, 212 p.
  22. Kishkin S.T., Polyak E.V. Fracture kinetics of heat-resistant alloys during creep. S.T. Kishkin. Development, investigation, and application of heat-resistant alloys. Selected works. Moscow: Nauka, 2006, pp. 92-105.
  23. Flemings M. Solidification processing. Trans. from Engl. Eds. A.A. Zhukov and B.V. Rabinovich. Moscow: Mir, 1977, 423 p.
  24. Stepanov V.M., Kishkin S.T., Chumakov V.A. et al. Advanced methods for precision casting of gas turbine engine blades. Aviation Materials. Moscow: ONTI, 1977, is. 1, pp. 8-80.
  25. Kablov E.N., Chubarov V.G. Casting of turbine blades from nickel-based alloys with an equiaxed polycrystalline structure. Cast Blades for Gas Turbine Engines: Alloys, Technologies, Coatings. Ed. by E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, pp. 187-234.
  26. Kandarov I.V., Pankratov D.L., Piksaev V.M. et al. Obtaining a fine-grained structure in large-sized blades made of heat-resistant nickel alloy IN792. Vestnik PNIPU. Mashinostroyenie. Materialovedeniye, 2022, vol. 24, no. 23, pp. 64-70. DOI: 10.15593/2224-9877/2022.3.08.
  27. Shalin R.E., Svetlov I.L., Kachanov E.B. et al. Single Crystals of Heat-Resistant Nickel Alloys. Moscow: Mashinostroenie, 1997, 336 p.
  28. Sengupta A., Putatunda S.K., Bartoslewcz L. et al. Tensile behavior of a new single-crystal nickel-based superalloy (CMSX-4) at room and elevated temperatures. Journal Materials Engineering and Performance, 1994, vol. 3 (1), pp. 73-81.
  29. Nathal M.V. Effect of initial gamma prime size on the elevated temperature creep properties in single crystal nickel base superalloys. Metallurgical Transactions A, 1987, vol. 18, is. 11, pp. 1961-1970.
  30. Kablov E.N., Evgenov A.G., Petrushin N.V. et al. Selective Laser Melting: Materials and Technologies for the Synthesis of Critical Components: A Textbook. Moscow: NRC «Kurchatov Institute» – VIAM, 2024, pp. 291–476.
  31. Sidorov V.V., Kablov D.E., Rigin V.E. Metallurgy of Heat-Resistant Casting Alloys: Technology and Equipment. Moscow: VIAM, 2014, 368 p.
  32. Vinarsky M.S., Lurie M.V. Design of Experiments in Technological Research. Kyiv: Tekhnika, 1975, 168 p.
  33. Kuleshova E.A., Kolotukhin E.V., Baryshev E.E. et al. Features of structure formation in the ZhS6U alloy after thermal-time treatment of the melt. Metallovedenie i termicheskaya obrabotka metallov, 1990, no. 11, pp. 61–64.
  34. Petrushin N.V., Cherkasova E.R. Dependence of phase transformation temperatures and structure of heat-resistant nickel alloys on melt heating temperature. Metallovedenie i termicheskaya obrabotka metallov,1993, no. 1, pp. 22–25.
  35. Zadgenidze I.G. Design of Experiments for the Study of Multicomponent Systems. Moscow: Nauka, 1976, 390 p.
  36. Draper N., Smith H. Applied Regression Analysis. Trans. from Engl. by Yu.P. Adler, V.G. Gorsky. 2nd ed. Moscow: Finansy i Statistika, 1986, 366 p.
  37. Iskhodzhanova I.V., Bondarenko Yu.A., Lapteva M.A. Evaluation of the structure of monocrystalline Ni superalloys derived in different conditions of directional solidification using methods of quantitative analysis of video images. Trudy VIAM, 2015, no. 12, pp. 46–54. Available at: http://www.viam-works.ru (accessed: July 20, 2026). DOI: 10.18577/2307-6046-2015-0-12-6-6.
  38. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Definition missfit in fragmental single crystals of nickel hot strength alloys. Trudy VIAM, 2013, no. 5, pp. 8–12. Available at: http://www.viam-works.ru (accessed: March 30, 2026).
  39. Gorelik S.S., Skakov Yu.A., Rastorguev L.N. X-ray and Electron-Optical Analysis. Moscow: MISiS, 2002, 358 p.
  40. Kuzmina N.A. Growth structural defects in single crystals of nickel heat-resistant alloys. Aviation materials and technologies, 2022, no. 3 (68), pp. 15–26. Available at: http://www.journal.viam.ru (accessed: April 22, 2026). DOI: 10.18577/2713-0193-2022-0-3-15-26.
  41. Starova E.N., Dolzhansky Yu.M., Sibileva L.I. et al. Processing and Analysis of Experimental Data on the Nairi-2 Computer: A Methodological Guide. Moscow: ONTI VIAM, 1979, 80 p.
  42. Kablov E.N., Golubovsky E.R. High-Temperature Strength of Nickel Alloys. Moscow: Mashinostroenie, 1998, 463 p.