A. B. Laptev, G. G. Matshov, N. I. Bulysheva, A. A. Krivushina, V. O. Startsev Toxicity of microparticles of paint coatings. Part 3. Risk assessment, regulation and prospective materials // Proceedings of VIAM. 2026. No. 7 (161). С. 177–192. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-177-192.

Toxicity of microparticles of paint coatings

Part 3. Risk assessment, regulation and prospective materials

A. B. Laptev1, G. G. Matshov2, N. I. Bulysheva2, A. A. Krivushina1, V. O. Startsev1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
2Federal Research Center Southern Scientific Center of the Russian Academy of Sciences, Rostov-on-Don, Russia; ssc-ras@ssc-ras.ru

Abstract

The final part of the series of articles is devoted to the assessment of toxicological risks, modern regulatory measures and the development of less dangerous paint and varnish coatings. Data on the toxicity of modern and promising paint compositions for ships is analyzed, and key dangerous components are identified. A microplastic pollution risk management plan is presented. Prospects of creating environmentally friendly coatings, including aqueous dispersions, biocide-free and hydrophobic antifouling coatings, and nanoparticle materials, are discussed.

Keywords
biocide, degradation of coatings, paints and varnishes, microplastics, polymer aging, toxicity, ecology
Reference list
  1. Occupational Exposures in Paint Manufacture and Painting. IARC Monographs on the Evaluation of Carcinogenic Risks to Humans, 1989, vol. 47, p. 324.
  2. Lead poisoning cases associated with environmental sources. Chemical Hazards and Poisons Report. Health Protection Agency, 2008, pp. 112–134.
  3. Dorne J.L., Kass G.E.N., Bordajandi L.R. et al. Human risk assessment of heavy metals: principles and applications. Metal Ions in Life Sciences, 2011, vol. 8, pp. 35–57.
  4. Silicone low friction-antifouling adhesive film for ships and manufacturing method thereof: pat. KR20230086093A; appl. 08.12.21; publ. 15.06.23.
  5. Recoating organosilicon acrylic finish paint with excellent weather resistance for ships: pat. CN101921537A (B); appl. 06.08.10; publ. 22.12.10.
  6. Environment-friendly water-based paint for ships: pat. CN111100488A; appl. 28.10.18; publ. 05.05.20.
  7. Alkyd paint for ships and preparation method: pat. CN101875811A (B); appl. 06.07.10; publ. 03.11.10.
  8. Bellas J. Comparative toxicity of alternative antifouling biocides to embryos and larvae of marine invertebrates. Science of the Total Environment, 2006, vol. 367, no. 2–3, pp. 573–585. DOI: 10.1016/j.scitotenv.2006.01.028.
  9. Antifouling paint for ships, as well as preparation method and application of antifouling paint: pat. CN107880603A; appl. 30.11.17; publ. 06.04.18.
  10. Long-acting waterborne ship interior paint and preparing method thereof: pat. CN109627936A (B); appl. 17.12.18; publ. 16.04.19.
  11. Antifouling paint for ships: pat. CN105778583A (B); appl. 21.03.16; publ. 20.07.16.
  12. Kennedy A.J., Hull M.S., Bednar A.J. et al. Fractioning nanosilver: importance for determining toxicity to aquatic test organisms. Environmental Science & Technology, 2010, vol. 44, no. 24, pp. 9571–9577. DOI: 10.1021/es1025382.
  13. Antifouling coating used for ships: pat. CN104342014A (B); appl. 23.10.14; publ. 11.02.15.
  14. Antifouling paint for ships and preparation method thereof: pat. CN116396684A (B); appl. 29.03.23; publ. 07.07.23.
  15. Over-rust corrosion protective coating for ships: pat. CN111100508A; appl. 28.10.18; publ. 05.05.20.
  16. Water-based anticorrosive paint for ships and preparation method of water-based anticorrosive paint: pat. CN116875139A (B); appl. 25.07.23; publ. 13.10.23.
  17. Antifouling coating for ship: pat. JP2014208823A (B2); appl. 16.07.07; publ. 06.11.14.
  18. Acid-resistant paint for ships: pat. CN114133832A; appl. 30.12.21; publ. 04.03.22.
  19. Epoxy acrylic joint paint for ships and preparation method of epoxy acrylic joint paint: pat. CN108034329A (B); appl. 30.11.17; publ. 15.05.18.
  20. Chubenko E.B., Baglov A.V., Dudchik N.V. et al. Evaluation of the integral toxicity of photocatalysts based on graphite-like carbon nitride in a luminescent test. Kinetika i kataliz, 2022, vol. 63, no. 2, pp. 187–192. DOI: 10.31857/S0453881122020010.
  21. Ye N., Wang Z., Wang S., Peijnenburg W.J. Toxicity of mixtures of zinc oxide and graphene oxide nanoparticles to aquatic organisms of different trophic level: particles outperform dissolved ions. Nanotoxicology, 2018, vol. 12, no. 5, pp. 423–438. DOI: 10.1080/17435390.2018.1458342.
  22. Bayouth J.E., Macey D.J., Kasi L.P., Fossella F.V. Dosimetry and toxicity of samarium-153-EDTMP administered for bone pain due to skeletal metastases. Journal of Nuclear Medicine, 1994, vol. 35, no. 1, pp. 63–69.
  23. Anticorrosive paint applied to ships and preparation method of anticorrosive paint: pat. CN114032003A (B); appl. 02.11.21; publ. 11.02.22.
  24. On approval of water quality standards for water bodies of fishery importance, including standards for maximum permissible concentrations of harmful substances in the waters of water bodies of fishery importance: Order of the Ministry of Agriculture of the Russian Federation dated 13.12.2016 No. 552. Available at: https://www.chemanalytica.ru/f/prikaz_minselkhoza_rossii_ot_13122016_n_552_ob_utverzhdenii_pdk.pdf (accessed: November 27, 2025).
  25. Halpern B.S., Walbridge S., Selkoe K.A. et al. A global map of human impact on marine ecosystems. Science, 2008, vol. 319, no. 5865, pp. 948–952. DOI: 10.1126/science.1149345.
  26. Gallo F., Fossi C., Weber R. et al. Marine litter plastics and microplastics and their toxic chemicals components: the need for urgent preventive measures. Environmental Sciences Europe, 2018, vol. 30, p. 13. DOI: 10.1186/s12302-018-0139-z.
  27. Bart J.C.J. Additives in Polymers: Industrial Analysis and Applications. Chichester: John Wiley & Sons, 2005, 594 p.
  28. Gallo F., Fossi C., Weber R. et al. Marine litter plastics and microplastics and their toxic chemicals components: the need for urgent preventive measures. Environmental Sciences Europe, 2018, vol. 30, art. 30.
  29. Weldon D.G. Failure Analysis of Paints and Coatings. Rev. ed. Chichester: John Wiley & Sons, 2009, 362 p.
  30. Wagner F., Rossi V., Aubry-Kientz M. et al. Pan-Tropical Analysis of Climate Effects on Seasonal Tree Growth. PLOS ONE, 2014, vol. 9, p. e92337. DOI: 10.1371/journal.pone.0092337.
  31. Koelmans A.A., Bakir A., Burton G.A., Janssen C.R. Microplastic as a Vector for Chemicals in the Aquatic Environment: Critical Review and Model-Supported Reinterpretation of Empirical Studies. Environmental Science & Technology, 2016, vol. 50, no. 7, pp. 3315–3326. DOI: 10.1021/acs.est.5b06069.
  32. Matishov G.G., Laptev A.B., Akhiyarov R.Zh. et al. Method of accounting for the accelerated destruction of coupon edges when determining the effectiveness of corrosion inhibitors. Corrosion Reviews, 2025, vol. 44 (1), p. 20240143. DOI: 10.1515/corrrev-2024-0143.
  33. Besseling E., Foekema E.M., van den Heuvel-Greve M.J., Koelmans A.A. The Effect of Microplastic on the Uptake of Chemicals by the Lugworm Arenicola marina (L.) under Environmentally Relevant Exposure Conditions. Environmental Science & Technology, 2017, vol. 51, no. 15, pp. 8795–8804. DOI: 10.1021/acs.est.7b02286.
  34. Wardrop P., Shimeta J., Nugegoda D. et al. Chemical Pollutants Sorbed to Ingested Microbeads from Personal Care Products Accumulate in Fish. Environmental Science & Technology, 2016, vol. 50, no. 7, pp. 4037–4044. DOI: 10.1021/acs.est.5b06280.
  35. Koelmans A.A., Besseling E., Foekema E.M. Leaching of plastic additives to marine organisms. Environmental Pollution, 2014, vol. 187, pp. 49–54. DOI: 10.1016/j.envpol.2013.12.013.
  36. Diepens N.J., Koelmans A.A. Accumulation of Plastic Debris and Associated Contaminants in Aquatic Food Webs. Environmental Science & Technology, 2018, vol. 52, no. 15, pp. 8510–8520. DOI: 10.1021/acs.est.8b02515.
  37. Hazimah N., Koelmans A.A. Transfer of PCBs from Microplastics under Simulated Gut Fluid Conditions Is Biphasic and Reversible. Environmental Science & Technology, 2019, vol. 53, no. 4, pp. 1871–1879. DOI: 10.1021/acs.est.8b05143.
  38. Lee H., Lee H.J., Kwon J.H. Estimating microplastic-bound intake of hydrophobic organic chemicals by fish using measured desorption rates to artificial gut fluid. Science of the Total Environment, 2018, vol. 642, pp. 505–513. DOI: 10.1016/j.scitotenv.2018.06.075.
  39. Beckingham B., Ghosh U. Differential bioavailability of polychlorinated biphenyls associated with environmental particles: Microplastic in comparison to wood, coal and biochar. Environmental Pollution, 2016, vol. 220, pp. 150–158. DOI: 10.1016/j.envpol.2016.09.033.
  40. Gassel M., Rochman C.M. The complex issue of chemicals and microplastic pollution: A case study in North Pacific lanternfish. Environmental Pollution, 2019, vol. 248, pp. 1000–1009. DOI: 10.1016/j.envpol.2019.02.067.
  41. Thompson R.C. Microplastics in the Marine Environment: Sources, Consequences and Solutions. Marine Anthropogenic Litter. Springer Open, 2015, pp. 185–200.
  42. Devriese L.I., De Witte B., Vethaak A.D., Leslie H.A. Bioaccumulation of PCBs from microplastics in Norway lobster (Nephrops norvegicus): An experimental study. Chemosphere, 2017, vol. 186, pp. 10–16. DOI: 10.1016/j.chemosphere.2017.07.121.
  43. Lohmann R. Microplastics are not important for the cycling and bioaccumulation of organic pollutants in the oceans – but should microplastics be considered POPs themselves? Integrated Environmental Assessment and Management, 2017, vol. 13, no. 3, pp. 460–465. DOI: 10.1002/ieam.1914.
  44. Kablov E.N., Sagomonova V.A., Sorokin A.E. et al. A Study of the Structure and Properties of Polymer Composite Materials with Integrated Vibration Absorbing Layer. Polymer Science, Series D, 2020, vol. 13, no. 3, pp. 335–340. DOI: 10.1134/S1995421220030090.
  45. Laptev A.B., Matishov G.G., Krivushina A.A., Pavlov M.R., Nikolaev E.V. The effect of the transition of air temperature through zero on the surface integrity of a polymer material. Part 1. Moistening. Trudy VIAM, 2025, no. 11 (153), pp. 147–156. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2025-0-11-147-156.
  46. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: November 27, 2025). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  47. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), pp. 32–51. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  48. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), pp. 114–122. Available at: http://www.viam-works.ru (accessed: November 27, 2025). DOI: 10.18577/2307-6046-2021-0-1-114-122.
  49. Bejarano A.C., Chandler G.T., Decho A.W. Influence of natural dissolved organic matter (DOM) on acute and chronic toxicity of the pesticides chlorothalonil, chlorpyrifos and fipronil on the meiobenthic estuarine copepod Amphiascus tenuiremis. Journal of Experimental Marine Biology and Ecology, 2005, vol. 321, no. 1, pp. 43–57. DOI: 10.1016/j.jembe.2005.01.005.
  50. ASTM E1688-19. Standard Guide for Determination of the Bioaccumulation of Sediment-Associated Contaminants by Benthic Invertebrates. West Conshohocken: ASTM International, 2019, 54 p.