V. A. Kuznetsova, V. V. Emelyanov, G. G. Shapovalov, V. G. Zheleznyak Research of protective properties of paint coatings during corrosion fatigue testing // Proceedings of VIAM. 2026. No. 7 (161). С. 167–176. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-167-176.

Research of protective properties of paint coatings during corrosion fatigue testing

V. A. Kuznetsova1, V. V. Emelyanov1, G. G. Shapovalov1, V. G. Zheleznyak1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The details of aviation engineering are characterized by cases of simultaneous influence of the corrosion environment and mechanical stresses which can arise at influence of permanent and alternating loads. The protective properties of systems of paint and varnish coatings, when testing for corrosion fatigue, and also to determination of adhesive durability of paint and varnish coatings at normal separation in initial condition and after cyclic tests for corrosion fatigue were studied. For tests, systems of coverings on the basis of disperse reinforced erosion-resistant enamels EP-5236 with different primers were selected in comparison with serial system of coverings on the basis of EP-140 enamel.

Keywords
paint coatings, durability at cyclic bend, durability at gap, elasticity of covering, adhesive durability, corrosion fatigue
Reference list
  1. History of Aviation Materials Science. VIAM - 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.
  2. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), pp. 62–67. Available at: http://www.viam-works.ru (accessed: January 14, 2026). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  3. Problems of protective paints and varnishes: Review of the materials of the European conference «Protective coating», Dusseldorf (Germany). Lakokrasochnye materialy i ikh primenenie, 2013, no. 9, pp. 33–35.
  4. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  5. Sosnina S.A., Kuleshova I.D. Regulation of the interaction of components in filled paint and varnish compositions. Lakokrasochnye materialy i ikh primenenie, 2011, no. 1, pp. 60–62.
  6. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex paint and varnish coating systems for the protection of metal polymer composite materials, as well as their contact joints from the effects of aggressive factors. Lakokrasochnye materialy i ikh primenenie, 2016, no. 6, pp. 32–35.
  7. Rosenfeld I.L., Rubinstein F.I., Zhigalova K.A. Protection of metals from corrosion with paint and varnish coatings. Moscow: Khimiya, 1987, 224 p.
  8. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), pp. 3–13. Available at: http://www.journal.viam.ru (accessed: February 10, 2026). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  9. Kondrashov E.K., Kozlova A.A. Efficiency of anticorrosive protection by organic silicon enamels of welded connections of VNS-2 and VNS-5 steels. Trudy VIAM, 2024, no. 3 (133), pp. 117–124. Available at: http://www.viam-works.ru (accessed: December 22, 2025). DOI: 10.18577/2307-6046-2024-0-3-117-124.
  10. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  11. Erasov V.S., Oreshko E.I. Mechanical testing and properties of structural aircraft metal materials: textbook. Ed. E.N. Kablov. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 344 p.
  12. Lutsenko A.N., Slavin A.V., Erasov V.S., Khvackij K.K. Strength tests and researches of aviation materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 527–546. DOI: 10.18577/2071-9140-2017-0-S-527-546.
  13. Kablov E.N., Khmeleva K.M., Zavarzin S.V., Kozlov I.A., Lonskii S.L. The effect of heat treatment on the characteristics of aluminium-zinc coatings obtained by the cold spray method. Aviation materials and technologies, 2022, no. 1 (66), pp. 78–91. Available at: http://www.journal.viam.ru (accessed: January 12, 2026). DOI: 10.18577/2713-0193-2022-0-1-78-91.
  14. Startsev O.V., Koval T.V., Krotov A.S., Dvirmaya E.V., Veligodsky I.M. Investigation of the properties of carbon fiber reinforced plastic with coatings after 8 and 13 years of aging in moderately warm climate. Part 2. Condition of protective paint and vanish coatings. Trudy VIAM, 2024, no. 11 (141), pp. 113–124. Available at: http://www.viam-works.ru (accessed: February 12, 2026). DOI: 10.18577/2307-6046-2024-0-11-113-124.
  15. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples' temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  16. Kuznetsova V.A. Influence of the elastomeric modifier on mechanical and viscoelastic properties of epoxy and rubber compositions for erosion resistant coatings. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 56–62. DOI: 10.18577/2071-9140-2020-0-2-56-62.
  17. Yulovskaya V.D. Oligomers. Rubber - oligomeric compositions, structure and properties: textbook. Moscow, 2008, 46 p.
  18. Rosenfeld I.L., Rubinstein F.I. Anticorrosive primers and inhibited paint and vanish coatings. Moscow: Khimiya, 1980, 196 p.
  19. Kuznetsova V.A., Deev I.A., Kuznetsov G.V., Kondrashov E.K. Effect of filler on the fatigue strength and microstructure of free-flowing polymer films under cyclic tension. Zavodskaya laboratoriya. Diagnostika materialov, 2014, vol. 80, no. 5, pp. 35–39.
  20. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  21. Smekhov F.M. Increasing the adhesive strength of coatings by regulating the polarity and segmental mobility of film-forming molecules. Lakokrasochnye materialy i ikh primenenie, 1986, no. 1, pp. 23–25.
  22. Sorokin M.F., Kochnova Z.A., Zakharova A.A., Golova N.A. Curing of epoxy oligomers with aminoalkoxysilanes. Lakokrasochnye materialy i ikh primenenie, 1986, no. 5, pp. 24–28.
  23. Chalykh A.E., Kochnova Z.A., Zhavoronok E.S. Compatibility and diffusion in epoxy oligomer – liquid carboxylate rubber systems. Vysokomolekulyarnyye soyedineniya. Seriya A, 2001, vol. 43, no. 12, pp. 1–9.
  24. Kablov E.N. The Role of Chemistry in the Creation of Next-Generation Materials for Complex Technical Systems. Abstracts of the Reports of the XX Mendeleev Congress on General and Applied Chemistry. UB of RAS, 2016, pp. 25–26.
  25. Shishelova T.I., Stepanova N.E., Plynskaya D.A., Belyaeva M.A. Whiskers. Uspekhi sovremennogo yestestvoznaniya, 2009, no. 8, pp. 12–13.
  26. Berlin A.A., Basin V.E. Basics of Polymer Adhesion. Moscow: Khimiya, 1969, 319 p.
  27. Semenova L.V., Nefedov N.I. Application of modified epoxy primers in the painting systems. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 38–44. DOI: 10.18577/2071-9140-2014-03-38-44.
  28. Kozlova L.S., Sibileva S.V., Chesnokov D.V., Kutyrev A.E. Corrosion inhibitors (review). Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 67–75. DOI: 10.18577/2071-9140-2015-0-2-67-75.
  29. Kochnova Z.A., Zhavoronok E.S., Kotova A.V. Features of the Production of Epoxy-Rubber Composites Based on Liquid Nitrile-Butadiene Rubbers and Epoxy Oligomers. Lakokrasochnye materialy i ikh primenenie, 1998, no. 11, pp. 27–28.
  30. Fabulyak F.G. Molecular Mobility in Surface Layers. Kyiv: Naukova Dumka, 1983, 144 p.
  31. Lipatov Yu.S. Interfacial Phenomena in Polymers. Kyiv: Naukova Dumka, 1980, 260 p.
  32. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  33. Kuznetsova V.A., Zheleznyak V.G., Silaeva A.A. Influence of mechanical characteristics of priming coverings on stability to cyclic mechanical loads of systems of the erosion resistant disperse reinforced coatings. Trudy VIAM, 2018, no. 6 (66), pp. 59–67. Available at: http://www.viam-works.ru (accessed: December 12, 2025). DOI: 10.18577/2307-6046-2018-0-6-59-67.