N. V. Petrushin, E. G. Rimsha, E. S. Elyutin, S. A. Lutskaya Iridium in single crystal nickel based superalloys with rhenium (review) // Proceedings of VIAM. 2026. No. 7 (161). С. 101–118. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-7-101-118.

Iridium in single crystal nickel based superalloys with rhenium (review)

N. V. Petrushin1, E. G. Rimsha1, E. S. Elyutin1, S. A. Lutskaya1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The analysis of the scientific and technical literature data on the influence of iridium on the structural phase characteristics, phase stability, and high temperature long term strength creep of single crystal Re- and Re–Ru-containing nickel based superalloys (NBSAs) has been carried out. It is established that the addition of iridium to rhenium-containing NBSAs is more effective than the addition of ruthenium, has a stabilizing effect on γ- and γʹ-phases, delaying the formation of harmful TCP phases in the temperature range of 900–1100 °C. As a result, single crystal rhenium containing NBSAs alloyed with iridium have a longer high-temperature creep life than alloys with ruthenium.

Keywords
single crystal nickel based superalloys, phase stability, TCP phase, long-term strength creep, iridium, ruthenium, rhenium
Reference list
  1. Petrushin N.V., Ospennikova O.G., Svetlov I.L. Single-crystal Ni-based superalloys for turbine blades of advanced gas turbine engines. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 72–103. DOI: 10.18577/2071-9140-2017-0-S-72-103.
  2. Elyutin E.S. Development of Heat-Resistant Nickel Alloys of Generations V and VI with Increased Long-Term Strength for Single-Crystal Blades of Advanced Aircraft Gas Turbine Engines: thesis abstract, Moscow, 2023, 28 p.
  3. Aviation Materials: reference book in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: NRC «Kurchatov Institute» – VIAM, 2022, vol. 3: Casting Heat-Resistant and Intermetallic Nickel-Based Alloys, 192 p.
  4. Walston S., Cetel A., MacKay R. et al. Joint development of a fourth generation single crystal superalloy. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 15–24.
  5. Caron P. High γ′ solvus new generation nickel-based superalloys for single crystal turbine blade applications. Superalloys 2000. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 737–746.
  6. Argence D., Vernault C., Desvallées Y., Fournier D. MC-NG: A 4th generation single-crystal superalloy for future aeronautical turbine blades and vanes. Superalloys 2000. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 829–837.
  7. Koizumi Y., Kobayashi T., Yokokawa T. et al. Development of next-generation Ni-base single crystal superalloys. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 35–43.
  8. Fifth generation nickel base single crystal superalloy TMS-196. Developed under NIMS/IHI collaboration. 2006. 4 p. Available at: http://sakimori.nims.go.jp (accessed: January 24, 2025).
  9. Sato A., Harada H., Yeh An-C. et al. A 5th generation SC superalloy with balanced high temperature properties and processability. Superalloys 2008. Pennsylvania: Minerals, Metals & Materials Society, 2008, pp. 131–138.
  10. Kawagishi K., Yeh An-C., Yokokawa T. et al. Development of an oxidation-resistant high-strength sixth-generation single-crystal superalloy TMS-238. Superalloys 2012. Pennsylvania: Minerals, Metals & Materials Society, 2012, pp. 189–195.
  11. Yokokawa T., Harada H., Kawagishi K. et al. Advanced alloy design program and improvement of sixth-generation Ni-base single crystal superalloy TMS-238. Superalloys 2020. Pennsylvania: Minerals, Metals & Materials Society, 2020, pp. 122–130. DOI: 10.1007/978-3-030-51834-9_12.
  12. Bondarenko Yu.A., Echin A.B., Surova V.A., Narsky A.R. Development of technologies and equipment for producing blades of the hot path of gas turbine engines from superalloys with directional and single-crystal structure. Trudy VIAM, 2023, no. 7 (125), pp. 3–14. Available at: http://www.viam-works.ru (accessed: November 28, 2025). DOI: 10.18577/2307-6046-2023-0-7-3-14.
  13. Svetlov I.L., Petrushin N.V., Zaitsev D.V. et al. Evolution of microstructure and phase composition of single crystals of nickel-based superalloy in the process of high-temperature creep. Physics of Metals and Metallography, 2025, vol. 126, no. 1, pp. 35–41. DOI: 10.1134/S0031918X24602592.
  14. Harada H. Development of Superalloys for 1700 °C ultra-efficient gas turbines. Proceedings of 9th Liege Conference «Materials for Advanced Power Engineering 2010». Belgium: University of Liège, 2010, pp. 604–614.
  15. Huang M., Zhu J. An overview of rhenium effect in single-crystal superalloys. Rare Metals, 2016, vol. 35, no. 2, pp. 127–139. DOI: 10.1007/s12598-015-0597-z.
  16. Neubauer C.M., Mari D., Dunand D.C. Diffusion in nickel-rhenium system. Scripta Metallugica at Materialia, 1994, vol. 31, no. 1, pp. 99–104. DOI: 10.1016/0956-716X(94)90102-3.
  17. Petrushin N.V., Svetlov I.L., Epishin A.I., Elyutin E.S. Development of directional solidification method to solve the problems of physical metallurgy of nickel- and cobalt-based superalloys. Part 2. Trudy VIAM, 2025, no. 6 (148), pp. 13–30. Available at: http://www.viam-works.ru (accessed: December 11, 2025). DOI: 10.18577/2307-6046-2025-0-6-13-30.
  18. Epishin A.I., Rodin A.O., Bokshteyn B.S., Svetlov I.L. Mutual diffusion in binary alloys of the Ni-Re system. Fizika metallov i metallovedenie, 2015, vol. 116, no. 2, pp. 184–190. DOI: 10.7868/S0015323015020138.
  19. Ding Q., Li S., Chen L.-Q. et al. Re segregation at interfacial dislocation network in nickel-base superalloys. Acta Materialia, 2018, vol. 154, pp. 137–146. DOI: 10.1016/j.actamat.2018.05.025.
  20. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaev M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 1. Aviation materials and technologies, 2023, no. 1 (70), pp. 30–50. Available at: http://www.journal.viam.ru (accessed: December 11, 2025). DOI: 10.18577/2713-0193-2023-0-1-30-50.
  21. Svetlov I.L., Petrushin N.V., Epishin A.I., Karashaev M.M., Elyutin E.S. Single crystals of nickel-based superalloys alloyed with rhenium and ruthenium (review). Part 2. Aviation materials and technologies, 2023, no. 2 (71), pp. 3–22. Available at: http://www.journal.viam.ru (accessed: December 11, 2025). DOI: 10.18577/2713-0193-2023-0-2-3-22.
  22. Matuszewski K., Rettig R., Singer R. The effect of Ru on precipitation of topologically close packed phases in Re-containing Ni base superalloys: quantitative FIB-SEM investigation and 3D image modeling. Proceedings of 2nd European Symposium on Superalloys and their Applications (Eurosuperalloys 2014). MATEC Web of Conferences, 2014, vol. 14. DOI: 10.1051/matecconf/20141409001.
  23. Yu X.X., Wang C.Y., Zhang X.N. et al. Synergistic effect of rhenium and ruthenium in nickel-base superalloys. Journal of Alloys and Compounds, 2004, vol. 51, pp. 327–331. DOI: 10.1016/j.jallcom.2013.07.201.
  24. Svetlov I.L., Petrushin N.V., Epishin A.I., Elyutin E.S. Synergistic effect of rhenium and ruthenium on the long-term strength of single crystals of nickel-based heat-resistant alloys of III–IV generations. Fizika metallov i metallovedenie, 2022, vol. 123, no. 8, pp. 888–894. DOI: 10.31857/S0015323022080137.
  25. Properties of the Elements: handbook in 2 parts. 2nd ed. Moscow: Metallurgy, 1976, part 1: Physical Properties, 600 p.
  26. Yuan Y., Kawagishi K., Koizumi Y. et al. Creep deformation of a 6th generation Ni-base single crystal superalloy at 800 °C and 735 MPa. Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 675–682.
  27. Pyczak F., Devrient B., Mughrabi H. The effects of different alloying elements on the thermal expansion coefficients, lattice constants and misfit of nickel-based superalloys investigated by X-ray diffraction. Superalloys 2004. Pennsylvania: Minerals, Metals & Materials Society, 2004, pp. 827–836.
  28. Wei B., Lin Y., Huang Z. et al. A novel Re-free Ni-based single-crystal superalloy with enhanced creep resistance and microstructure stability. Acta Materialia, 2022, vol. 240, art. 118336. DOI: 10.1016/j.actamat.2022.118336.
  29. Honeycomb R. Plastic Deformation of Metals. Moscow: Mir, 1972, 408 p.
  30. Phase Diagrams of Binary Metallic Systems: A Handbook in 3 vols. Moscow: Mashinostroenie, 1999, vol. 3, book 1, 872 p.
  31. Barabash O.M., Koval Yu.N. Crystal Structure of Metals and Alloys. Kyiv: Naukova Dumka, 1986, 598 p.
  32. Velikanova T.Ya., Mazhuga T.G., Semonova O.L. et al. Phase Diagram of the Ni-Os System. Metallurgical Metal Ceramics, 2002, vol. 41 (5–6), pp. 288–295.
  33. Okamoto H. Ni-Os (Nickel-Osmium). Journal Equilibria and Diffusion, 2009, vol. 30, p. 662. Available at: https://himikatus.ru/art/phase-diagr1/Ni-Os (accessed: December 22, 2025).
  34. Bokshteyn B.S., Bokshteyn S.Z., Zhukhovitsky A.A. Thermodynamics and kinetics of diffusion in solids. Moscow: Metallurgiya, 1974, 279 p.
  35. Murakami H., Honma T., Koizumi Y., Harada H. Distribution of platinum group in Ni-base single-crystal superalloys. Superalloys 2000. Pennsylvania: Minerals, Metals & Materials Society, 2000, pp. 747–756.
  36. Reed R.C., Yeh A.C., Tin S. et al. Identification of the partitioning characteristics of ruthenium in single crystal superalloys using atom probe tomography. Scripta Materialia, 2004, vol. 51, pp. 327–333. DOI: 10.1016/j.scriptamat.2004.04.019.
  37. Mori Y., Yokokawa T., Kobayashi T. et al. Microstructure and creep strength of the Ni-base single crystal superalloys containing Ir substituting for Ru. The 9th Pacific Rim International Conference on Advanced Materials and Processing (PRICM9). The Japan Institute of Metals and Materials, 2016, pp. 765–769.
  38. Murakami H., Osawa M., Yokokawa T. et al. The location of atoms in Ir-containing Ni-base single-crystal superalloys. Materials for Advanced Power Engineering 1998: Proceeding of the 6th Liége Conference. Universite de Liége, 1998, pp. 1139–1145.
  39. Yokokawa T., Osawa M., Nishida K. et al. Partitioning behavior of platinum group metals on the γ and γ′ phases of Ni-base superalloys at high temperatures. Scripta Materialia, 2003, vol. 49, pp. 1041–1046.
  40. Kobayashi T., Koizumi Y., Nakazawa S. et al. Design of high rhenium containing single-crystal superalloys with balanced intermediate and high temperature creep strengths. Proceedings of the Fourth International Charles Parsons Turbine Conference on «Advances in Turbine Materials, Design and Manufacturing». Newcastle upon Tyne, UK, 1997, pp. 766–773. Available at: https://sakimori.nims.go.jp/documents/990225c.html (accessed: December 11, 2025).
  41. Mori Y., Yokokawa T., Kobayashi T. et al. Phase stability of nickel-base single-crystal superalloys containing iridium substituting for ruthenium. Materials Transactions, 2016, vol. 57, pp. 1845–1848. DOI: 10.2320/matertrans.MAW201606.
  42. Utada S., Yokokawa T., Kobayashi T. et al. Challenging the limit of strengthening by γ/γ′ lattice misfit on the high temperature creep properties of Ni-base single crystal superalloy. Metallurgical and Material Transaction A, 2026, vol. 57, pp. 1794–1812. DOI: 10.1007/s11661-025-08089-5.
  43. Karunaratne M.S.A., Reed R.C. Interdiffusion of the platinum group metals in nickel at elevated temperatures. Acta Materialia, 2003, vol. 51, is. 10, pp. 2905–2919. DOI: 10.1016/S1359-6454(03)00105-8.
  44. Estulin G.V., Svistunova T.V. The influence of rhenium and iridium on the properties of heat-resistant nickel alloys. Study of steel and alloys. Moscow: Nauka, 1964, pp. 194–198.
  45. Yokokawa T., Harada H., Mori Y. et al. Design of next generation Ni-base single-crystal superalloy containing Ir: towards 1150 °C temperature capability. Superalloys 2016. Pennsylvania: Minerals, Metals & Materials Society, 2016, pp. 123–130.